Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C @Thickness 3.20 mm |
333 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP KONDUIT ITF2B PA 6/12 (Asia Pacific) LNP* Konduit* ITF2B is a compound based on Nylon 6/12 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C @Temperature 200 °C, Time 14400 sec |
333 °F @Temperature 392 °F, Time 4.00 hour |
ISO 75A-f |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C @Temperature 200 °C, Time 14400 sec |
333 °F @Temperature 392 °F, Time 4.00 hour |
Annealed; ISO 75A-f |
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | ASTM D648 |
Gharda Chemicals Gafone S S1430SP60 Polysulfone (PS)
(discontinued **) Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific) LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP GX07409H PSU LNP* LUBRICOMP* GX07409H is a compound based on PSU resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Healthcare. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp GX07409X PSU Wear resistant PSUThis data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0254 C 75% Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium Sulfate, 75% Filler by WeightFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0266 B Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0303 B Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityAppearance: Natural Color and WhiteInformation provided by TP Composites, Inc... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0390 BK Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Europe-Africa-Middle East) LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C @Thickness 3.20 mm |
333 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU (Asia Pacific) LNP* Thermocomp* GX05482 is a compound based on Polysulfone resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0180 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0201 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0232 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0348 Availability: North AmericaForms: PelletsFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0365 01 BK Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0365 BK Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0388 Availability: North AmericaForms: PelletsFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0425 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 0445 A Availability: North AmericaForms: PelletsFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | ASTM D648 |
Plenco 4311 Phenolic, Granular, Injection Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | ISO 75 |
BASF Ultrason S 2010 PSU Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | ASTM D648 |
Toyobo T-751 Nylon, Painting Grade Key Feature: Glass fiber and mineral reinforced, high heat distortion and impact gradesInformation provided by Toyobo Co., Ltd |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | ASTM D648 |
Plenco 2311 Phenolic, Granular, Transfer Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 167 °C | 333 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas re.. |