Plastcom SLOVAMID 6 BT LS Polyamide 6, UV Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Plastcom SLOVAMID 6 BT LS Polyamide 6, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesPA 6 for injection moulding with the content of UV stabilizer predetermines products for external use, eg. seats for sport stadiums, covers of electrical appliances. Delivered in natural and in the full RAL color scale.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
STN 64 0111
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
STN 64 0808
Linear Mold Shrinkage, Transverse 0.0183 cm/cm
0.0183 in/in
STN 64 0808
Melt Flow 6.0 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
6.0 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.0 MPa
11900 psi
STN EN ISO 527-2
Elongation at Break 4.0 %
4.0 %
STN EN ISO 527-2
Tensile Modulus 3.00 GPa
435 ksi
STN EN ISO 527-2
Flexural Strength 115 MPa
16700 psi
STN EN ISO 178
Flexural Modulus 2.60 GPa
377 ksi
STN EN ISO 178
Charpy Impact Unnotched 7.50 J/cm²
<br>@Temperature -20.0 °C
35.7 ft-lb/in²
<br>@Temperature -4.00 °F
STN EN ISO 179
12.0 J/cm²
<br>@Temperature 23.0 °C
57.1 ft-lb/in²
<br>@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 0.150 J/cm²
<br>@Temperature 23.0 °C
0.714 ft-lb/in²
<br>@Temperature 73.4 °F
STN EN ISO 179
0.150 J/cm²
<br>@Temperature -20.0 °C
0.714 ft-lb/in²
<br>@Temperature -4.00 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
DSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
STN EN ISO 75/A
Vicat Softening Point 190 °C
374 °F
B; STN EN ISO 306
Flammability, UL94 HB
HB
Glow Wire Test 960 °C
1760 °F
STN IEC 60695-2-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
STN IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
STN IEC 60093
Dielectric Strength 18.0 kV/mm
457 kV/in
STN IEC 60243
Comparative Tracking Index 600 V
600 V
STN 34 6468
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
STN EN ISO 960
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi