Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Premix Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-15 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | in oil; ASTM D149 |
PTS PBT-20GFR 20% Glass Filled PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by PTS LLC. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® R-4 02 Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at elev.. |
|||
Dielectric Strength | 18.0 - 34.0 kV/mm | 457 - 864 kV/in | Average value: 26.2 kV/mm Grade Count:5 |
Overview of materials for Nylon 11, Flexible Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 45GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.59 mm |
457 kV/in @Thickness 0.0625 in |
Perpendicular, Short Time in Oil and Air; ASTM D149 |
Haysite ETR-FR-C Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) ETR-FR-C meets NEMA GPO-3 requirements and exceeds NEMA in dielectric strength, arc resistance, and track resistance. This U.L. recognized grade is highly flame retardant and low smoke generating. E.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | IEC 60243 |
Solvay TECHNYL® C 230 PA6, Conditioned Description: Unreinforced polyamide PA6, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: This grade has improved impact strength and higher flexibili.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | GB/T1408.1-2006 |
Sichuan Deyang Haton® hFR81 Polyphenylene Sulfide Injection molding, reinforcedInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Samyang Tribit® 1501N PBT, Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1501N is a V-2 flame retardancy grade.Appli.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 2.00 mm |
457 kV/in @Thickness 0.0787 in |
ASTM D149 |
UBE UPIMOL® R Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149-95a |
Thermoseal KLINGERSIL® C-4300 General Application Gasketing Synthetic FiberNitrile BinderGood SealabilityGood Chemical ResistanceGeneral Purpose SheetInformation provided by Thermoseal Inc. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | Insulating Strength |
China-Yixing Longly Refractories 99 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | |
AGY ZenTron® S-2 Generic S-Glass Fiber S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod.. |
|||
Dielectric Strength | 18.0 - 36.0 kV/mm | 457 - 914 kV/in | Average value: 22.7 kV/mm Grade Count:29 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 2.00 mm |
457 kV/in @Thickness 0.0787 in |
IEC 60243 |
Manifattura Cattaneo POM c+PTFE Acetal, PTFE Filled Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |