Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 56 FRD 1 Polypropylene Homopolymer, Halogen Flame Retardant FeaturesModified homopolymer PP for injection moulding with increased flammability resistance. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil form.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 BT Polyamide 6 FeaturesBasic type PA 6 for injection moulding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical .. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 FRC 2 LI PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 FRC 2 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization FeaturesLongterm external use is possible because of the material stabilization with the light stabilizers on the HALS basis. Meets the flammability in accordance with the norm DIN 4102 - B1. PA 6.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 FRC 2 Polyamide 6, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electro-technical purposes. Excellent flow of the material predetermines.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 NGR PA6, basic type FeaturesPA 6 for injection moulding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, faste.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 BT LS Polyamide 6, UV Stabilized FeaturesPA 6 for injection moulding with the content of UV stabilizer predetermines products for external use, eg. seats for sport stadiums, covers of electrical appliances. Delivered in natural an.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature -30.0 °C |
57.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® K223-KM6 Nylon 6-30% Mineral Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature -20.0 °C |
57.1 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 2-2120 17TOP BU UV-Stabilized 17% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-2120 17TOP BU is a black colored, 17% talc-filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-2120 17TOP BU is developed for producing injection .. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Ineos ABS Lustran® ABS E112LG Pellets Lustran® ABS E112LG is extrusion grade for low gloss surfaces. It is used for the production of molded plastic articles. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature -30.0 °C |
57.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Novodur® H701 ABS Novodur H701 is an injection molding grade of ABS with heat resistance and high impact strength.Information provided by Styrolution |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature -30.0 °C |
57.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eU |
Styrolution Novodur® P2M-V ABS Pellets Novodur® P2M-V has high impact strength, high gloss, and low emission. It is used for the production of molded plastic articles. |
|||
Charpy Impact Unnotched | <= 12.0 J/cm² @Temperature -30.0 °C |
<= 57.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Styrolution Polystyrol 454 C GR 2 PS Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution PS 456EB HIPS Styrolution PS 456EB is a high flow, high impact polystyrene with a good heat resistance and a high stiffness, developed for injection blow molding applications, especially for bottle of yot.High fl.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution PS 576H HIPS Styrolution PS 576H is a high gloss, high impact polystyrene with a good flow and good heat resistance.High gloss HIPSGood flow and heat resistanceHIPS with good balance of mechanical properties and.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature -30.0 °C |
57.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Terlux® 2802 TR Q434 Transparent MABS Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Terlux® 2812 HD MABS Description: Terlux 2812 HD is a suitable grade for the food packaging and health care and diagnostic markets.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Terlux® HD 2822 MABS Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well .. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Borealis Daplen™ EF267AI Polypropylene TPO Compound Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature -30.0 °C |
57.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
DIN ISO 179 |
BASF Elastollan R 3000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 FRC 2 TS PA6, flame retardant, heat stability FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature -30.0 °C |
57.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Durethan® DP 2801 000000 Nylon 66 PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature -30.0 °C |
57.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Pocan® S 7020 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified |