Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Murtfeldt Material ”S”® 1000 Green Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Murtfeldt Kunststoffe GmbH & Co
Trade Name Material ”S”®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Murtfeldt Material ”S”® 1000 Green Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compression-molded at high pressure and temperatures to form new semi-finished products. This results in a high-quality material with an exceptional price/performance ratio that is characterized by exceptional abrasion resistance and good slide properties.Special Properties:• Physiologically safe• Good wear resistance properties• Good slide properties• Good anti-adhesion properties• No moisture absorption• Electrically isolatingInformation provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density <= 0.940 g/cc
<= 0.0340 lb/in³
ISO 1183
Moisture Absorption at Equilibrium <= 0.010 %
<= 0.010 %
ISO 62
Water Absorption at Saturation <= 0.010 %
<= 0.010 %
ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 61 - 65
61 - 65
DIN 53505
Ball Indentation Hardness 38.0 MPa
5510 psi
Tensile Strength 23.5 MPa
3410 psi
ISO 527
Tensile Strength, Yield >= 15.0 MPa
>= 2180 psi
ISO 527
Elongation at Break 360 %
360 %
ISO 527
Modulus of Elasticity 0.950 GPa
138 ksi
Compressive Yield Strength 6.00 MPa

@Strain 1.00 %
870 psi

@Strain 1.00 %
ISO 604
10.5 MPa

@Strain 2.00 %
1520 psi

@Strain 2.00 %
ISO 604
18.0 MPa

@Strain 5.00 %
2610 psi

@Strain 5.00 %
ISO 604
Charpy Impact, Notched >= 8.00 J/cm²
>= 38.1 ft-lb/in²
ISO 179
Coefficient of Friction, Dynamic 0.10 - 0.20
0.10 - 0.20
Sand Slurry 120
120
value in %
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 23.0 - 60.0 °C
111 µin/in-°F

@Temperature 73.4 - 140 °F
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
ISO 52612
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146
Maximum Service Temperature, Air 90.0 °C
194 °F
Short Term
80.0 °C

@Time 1.80e+7 sec
176 °F

@Time 5000 hour
Minimum Service Temperature, Air -150 °C
-238 °F
Glass Transition Temp, Tg -120 °C
-184 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
IEC 60093
Dielectric Strength <= 45.0 kV/mm
<= 1140 kV/in
IEC 60243
Compliance Properties Metric English Comments
FDA No
No
Descriptive Properties Value Comments
Color Green