Thermal Properties Metric English Comments
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Material ”S”® 1000 Black Antistatic Polyethylene, Conductive
Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Material ”S”® 1000 Green Polyethylene
Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Material ”S”® 1000 RB Polyethylene, High Friction
An elastomer in Material ”S”® 1000 RB gives it high impact resistance and skid resistance.Special Properties:• High coefficient of friction• Good wear and abrasion resistanceInformation provide..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Muralen® plus + AB Polyethylene, Antibacterial
Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Muralen® Polyethylene
Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive
Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Original Material ”S”® Green Polyethylene
Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial
Material ”S”® plus + AB contains special substances that prevent the growth of bacteria and other microbes. The material is thus ideally suited for use when manufacturing and processing foods.Sp..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Original Material ”S”® plus + Bright ESD Polyethylene, Conductive
Material ”S”® plus+ Bright ESD is a light plastic with high conductivity and a voltage-dissipating effect on earthed components. This material is ideal for use in applications where a high value..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Original Material ”S”® plus + ESD Polyethylene, Conductive
Material ”S”® plus+ ESD has extremely low electrical resistance and is an optimum conductor. Full voltage dissipation for earthed components at maximum speed enables safe, spark-free work. This m..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled
The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from ..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction
This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan..
Glass Transition Temp, Tg -120 °C
-184 °F
Murtfeldt Original Material ”S”® plus + TLS Polyethylene
Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i..
Glass Transition Temp, Tg -120 - 118 °C
-184 - 244 °F
Average value: -104 °C Grade Count:29
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Glass Transition Temp, Tg -120 - 118 °C
-184 - 244 °F
Average value: -106 °C Grade Count:37
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
Glass Transition Temp, Tg -120 °C
-184 °F
Trelleborg Emerson & Cuming Stycast® 5954 Two-Component Silicone High Service Temp Encapsulant
Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har..
Glass Transition Temp, Tg -120 °C
-184 °F
Ultimate Tg
Tra-Con Tra-Bond 813J01 Silicone Encapsulant
TRA-BOND 813J01 is a silicone adhesive system formulated to provide excellent thermal conductivity. This unique product bonds well to difficult substrates. Typical applications include encapsulation..
Glass Transition Temp, Tg -120 °C
-184 °F
Silicone Property; ASTM D3418
Arlon Thermabond® 99A60X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Glass Transition Temp, Tg -120 °C
-184 °F
Silicone Property; ASTM D3418
Arlon Thermabond® R37300X008 0.008" Uncured Silicone Rubber on Fiberglass Carrier
Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m..