Momentive Performance Materials Electro 170 Heat Cured Rubber - High Voltage Insulating

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials Electro 170 Heat Cured Rubber - High Voltage Insulating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.Electro 170 is a specialty grade, peroxide curable silicone elastomer.Key Feature: Excellent Tracking and erosion resistance (1a 4.5KV); improved hydrophobicity
Physical Properties Metric English Comments
Specific Gravity 1.57 g/cc
1.57 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength 5.50 MPa
798 psi
Elongation at Break 250 %
250 %
Tear Strength 16.0 kN/m
91.3 pli
Die B
Descriptive Properties Value Comments
Appearance Grey