Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 23.5 MPa | 3410 psi | ISO 527 |
Murtfeldt Material ”S”® 1000 Green Polyethylene Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio.. |
|||
Tensile Strength | 23.5 MPa | 3410 psi | ISO 527 |
Gromax 1155LL TPE 1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex.. |
|||
Tensile Strength | 23.5 MPa | 3410 psi | perpendicular to plane; ASTM C297 |
3A Composites Core Materials BALTEK® SB.150 Structural End-Grain Balsa BALTEK SB is a core material produced from certified kiln-dried balsa wood in the ‘end-grain’ confiation. It has extremely high strength and stiffness to weight ratios, and achieves an excellent b.. |
|||
Tensile Strength | 23.5 MPa | 3410 psi | ASTM D638M |
Asia Technology Pioneers CAP 502 PP Nanocomposite Description: CAP502 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |