Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | <= 45.0 kV/mm | <= 1140 kV/in | IEC 60243 |
Murtfeldt Material ”S”® 8000 Polyethylene Material ”S”® 8000 improves on the already impressive material properties of Original Material ”S”®. The self lubricating character of this material makes it ideally suited for use in sliding.. |
|||
Dielectric Strength | <= 45.0 kV/mm | <= 1140 kV/in | IEC 60243 |
Murtfeldt Muralen® Polyethylene Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Dielectric Strength | <= 45.0 kV/mm | <= 1140 kV/in | IEC 60243 |
Murtfeldt Original Material ”S”® Natural Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® natural has excell.. |
|||
Dielectric Strength | <= 45.0 kV/mm | <= 1140 kV/in | IEC 60243 |
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | ISO.243 DIN.53481 |
Omnia Plastica PE 1000 - Polyethylene 1000 Polyethylene with a molecular weight of ± 1000,000 with excellent impact strength. PE 1000 is less rigid and has a higher shock resistance than the low molecular weight polyethylene and it is there.. |
|||
Dielectric Strength | >= 45.0 kV/mm | >= 1140 kV/in | ISO.243 DN.53481 |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data) TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
Quadrant EPP TIVAR® TECH PE-UHMW + MoS2 (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains molybdenum disulphide, resulting in a material with improved wear resistance and sliding properties over TIVAR 1000. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 60243-1 |
PolyOne Bergamid™ AB700 UF SO Polyamide 66/6 Copolymer (Nylon 66/6) Information provided by PolyOne |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 60243-1 |
PolyOne Bergamid™ B700 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Dielectric Strength | 45.0 kV/mm @Thickness 2.00 mm |
1140 kV/in @Thickness 0.0787 in |
IEC 60243 |
Manifattura Cattaneo PE UMW Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | VDE 0303 |
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight The ultra high molecular weight Polyethylene has a high abrasion resistance and a high toughness at the same time. The chemical and the crack resistance are optimized in comparison to the standard P.. |
|||
Dielectric Strength | 45.0 - 90.0 kV/mm | 1140 - 2290 kV/in | DIN 53481 |
Isoflon PEHD 500 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Dielectric Strength | >= 45.0 kV/mm | >= 1140 kV/in | in air, molded; ASTM D149 |
Guarniflon PTFE G500 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
Dielectric Strength | 45.0 kV/mm @Thickness 1.00 mm |
1140 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Bayblend® T80 XG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Opt.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® 2SV-30H black 9992 PA610-GF30 Product Description: GRILAMID XE 3976 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4104 nat PA610-GF40 Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | ASTM D877 |
ExxonMobil 18M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Dielectric Strength | >= 45.0 kV/mm | >= 1140 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PMMA Components made of PMMA are brilliantly transparent. Outstanding aging stability and weathering resistance. Good surface hardness. Abrasion-resistant. Physiologically safe. High strength. Easi.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
ExxonMobil Univis N 32 UNIVIS N hydraulic oils are high-performance anti-wear fluids designed to meet the needs of all major manufacturers and users of hydraulic equipment. They feature high viscosity indexes (VIs), obtai.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TR 90 NZZ nat PAMACM12-I Product description: Grilamid TR 90 NZZ natural is an amorphousthermoplastic polyamide, based on aliphatic and cycloaliphatic units. Grilamid TR 90 NZZ natural offers a variety of interesting proper.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4217 black 9233 PA6T/66-GF45 Product description: Grivory XE 4217 black 9233 is a high heat stabilized, 45% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection moulding. Polymer designation.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 60243-1 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |