Polymer Property : Minimum Service Temperature, Air = -238 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -150 °C
-238 °F
Murtfeldt Material ”S”® 1000 Black Antistatic Polyethylene, Conductive
Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio..
Minimum Service Temperature, Air -150 °C
-238 °F
Murtfeldt Material ”S”® 1000 Green Polyethylene
Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio..
Minimum Service Temperature, Air -150 °C
-238 °F
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive
Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro..
Minimum Service Temperature, Air -150 °C
-238 °F
Murtfeldt Original Material ”S”® plus + Bright ESD Polyethylene, Conductive
Material ”S”® plus+ Bright ESD is a light plastic with high conductivity and a voltage-dissipating effect on earthed components. This material is ideal for use in applications where a high value..
Minimum Service Temperature, Air -150 °C
-238 °F
Murtfeldt Original Material ”S”® plus + ESD Polyethylene, Conductive
Material ”S”® plus+ ESD has extremely low electrical resistance and is an optimum conductor. Full voltage dissipation for earthed components at maximum speed enables safe, spark-free work. This m..
Minimum Service Temperature, Air -150 °C
-238 °F
Quadrant EPP Cestilene™ HD 1000 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Minimum Service Temperature, Air -150 °C
-238 °F
Quadrant EPP Cestlite™ ASTL Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Minimum Service Temperature, Air -150 °C
-238 °F
GEHR Plastics PE-UHMW-ELS Polyethylene  (discontinued **)
Polyethylene offers resistance to almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature of HDPE is from -58 °F to +1..
Minimum Service Temperature, Air -150 °C
-238 °F
Manifattura Cattaneo PE UMW Polyethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Minimum Service Temperature, Air -150 °C
-238 °F
GEHR Plastics PE-UHMW Polyethylene, Ultra High Molecular Weight
The ultra high molecular weight Polyethylene has a high abrasion resistance and a high toughness at the same time. The chemical and the crack resistance are optimized in comparison to the standard P..
Minimum Service Temperature, Air -150 °C
-238 °F
Isoflon Tisoflon® 3G Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Minimum Service Temperature, Air -150 °C
-238 °F
Isoflon Tisoflon® 5G Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Minimum Service Temperature, Air -150 °C
-238 °F
Isoflon Tisoflon® 6 AD EXTRA SMOOTH Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.
Minimum Service Temperature, Air -150 °C
-238 °F
Isoflon Tisoflon® 6G EXTRA SMOOTH QUALITY Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Minimum Service Temperature, Air -150 °C
-238 °F
Isoflon Tisoflon® 10 AD Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.
Minimum Service Temperature, Air -150 °C
-238 °F
Isoflon Tisoflon® 10G Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Minimum Service Temperature, Air -150 °C
-238 °F
Isoflon Tisoflon® 14 AD Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.
Minimum Service Temperature, Air -150 °C
-238 °F
Isoflon Tisoflon® 14G Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Minimum Service Temperature, Air -150 °C
-238 °F
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.
Minimum Service Temperature, Air -150 °C
-238 °F
Isoflon Tisoflon® 5 AD Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.
Minimum Service Temperature, Air -150 °C
-238 °F
Continuous
Isoflon MFA TFE/Perfluoromethylvinylether Copolymer
Fluoropolymer material specifications.Information provided by Isoflon.