Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LDPE 2501TN00 Hygienic Film It is used in diaper film, lamination film and in applications where low blocking behavior without the help of additives is required.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ISO 1183
Melt Flow 0.75 g/10 min
0.75 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO R527-1
Film Tensile Strength at Yield, TD 12.0 MPa
1740 psi
ISO R527-1
Film Elongation at Break, MD >= 200 %
>= 200 %
ISO R527-1
Film Elongation at Break, TD >= 500 %
>= 500 %
ISO R527-1
Modulus of Elasticity 0.190 GPa
27.6 ksi
MD; ISO R527-1
0.200 GPa
29.0 ksi
TD; ISO R527-1
Tensile Impact 200 J/cm
375 ft-lb/in
ASTM D4272
Coefficient of Friction 0.70
0.70
ASTM D1894
Tear Strength 30.0 kN/m
171 pli
TD; ISO 6383-2
35.0 kN/m
200 pli
MD; ISO 6383-2
Film Tensile Strength at Break, MD 28.0 MPa
4060 psi
ISO R527-1
Film Tensile Strength at Break, TD 25.0 MPa
3630 psi
ISO R527-1
Optical Properties Metric English Comments
Haze 10 %
10 %
ASTM D1003A
Gloss 50 %
50 %
ASTM D2457
Descriptive Properties Value Comments
Clarity, mV 34
Sabtec