Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | <= 45.0 kV/mm | <= 1140 kV/in | IEC 60243 |
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial Material ”S”® plus + AB contains special substances that prevent the growth of bacteria and other microbes. The material is thus ideally suited for use when manufacturing and processing foods.Sp.. |
|||
Dielectric Strength | >= 45.0 kV/mm | >= 1140 kV/in | ISO.243 DN.53481 |
Polimersan Plastics POLIPOLEN® (Polyethylene) UHMW-PE 1000 PE 1000: Polyethylene with very high molecular weight (UHMW - PE 1000; Ultra High Molecular Weight Polyethylene). Polyethylenes with molecular weight higher than 3 million gr/mol. POLIPOLEN® PE (P.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
Quadrant EPP TIVAR® TECH PE-UHMW + MoS2 (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains molybdenum disulphide, resulting in a material with improved wear resistance and sliding properties over TIVAR 1000. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 60243-1 |
Polymer Industries Polyslick UHMW Profile Polyslick UHMW Profiles exhibit all of the durable qualities of our Polyslick UHMW Sheet making them perfect for use where sheet stock is not suitable. Polymer Industries offers a large variety of p.. |
|||
Dielectric Strength | 45.0 kV/mm @Thickness 2.00 mm |
1140 kV/in @Thickness 0.0787 in |
IEC 60243 |
Manifattura Cattaneo PE HD Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Dielectric Strength | 45.0 kV/mm @Thickness 2.00 mm |
1140 kV/in @Thickness 0.0787 in |
IEC 60243 |
Manifattura Cattaneo PE UMW Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 243 |
LG Chemical XR-472 ABS, High Heat Resistance, High Gloss Information Provided by LG Chem |
|||
Dielectric Strength | 45.0 - 90.0 kV/mm | 1140 - 2290 kV/in | DIN 53481 |
Isoflon PEHD 1000 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Dielectric Strength | 45.0 - 90.0 kV/mm | 1140 - 2290 kV/in | DIN 53481 |
Isoflon PEHD 500 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | ASTM D877 |
ExxonMobil 18M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LBV-30H FWA black 9225 PA12-GF30 Product Description: Grilamid LBV-30H FWA black 9225 is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined wit.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4104 nat PA610-GF40 Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | ASTM D877 |
ExxonMobil 13M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Dielectric Strength | >= 45.0 kV/mm | >= 1140 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PBT Polybutylene Terephthalate The mechanical properties of PBT are generally inferior to the partially crystallized PET, however, PBT is more easily machined.Information provided by Hippe. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PE 1000 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LBV-30H FWA nat PA12-GF30 Product Description: Grilamid LBV-30H FWA natural is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 60243-1 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | |
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | in transformer oil; IEC 60243-1 |
CENTROPLAST CENTROLEN PE-HD Polyethylene high density This material is a low density, easily machined plastic that can be welded and has good chemical resistance. Applications include apparatus engineering, and machines in the foodstuff industry.Infor.. |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Dielectric Strength | 45.0 kV/mm | 1140 kV/in | in transformer oil; IEC 60243-1 |
CENTROPLAST CENTROLEN PE-UHMW Ultra-high molecular weight polyethylene This plastic is a low density, easily machined material that can be welded and has a low sliding friction with high impact resistance. Applications include glide strips, pump components, and wearin.. |