Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | >= 8.00 J/cm² | >= 38.1 ft-lb/in² | ISO 179 |
Murtfeldt Material ”S”® 1000 Green Polyethylene Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO179/3C DIN.53453 |
Omnia Plastica PE 1000 - Polyethylene 1000 Polyethylene with a molecular weight of ± 1000,000 with excellent impact strength. PE 1000 is less rigid and has a higher shock resistance than the low molecular weight polyethylene and it is there.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 133R PC (Europe-Africa-Middle East) LEXAN 133R is the highest viscosity, UV stabilized, release containing, linear polycarbonate grade. Suitable for injection molding and extrusion processes. Available in transparent and multiple colo.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 134R PC (Europe-Africa-Middle East) LEXAN 134R is a high viscosity grade especially suited for injection blow moulding. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP SMC 0180 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 0400 Unsaturated Polyester UP SMC 0400 is a Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to parts with good up to excellent surface quality for medium bake in-line and off-line p.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 1500 Unsaturated Polyester UP SMC 1500 is a special SMC for applications calling for high continuous service temperature. The glass level has been selected to combine good mouldability with good strength and stiffness properties.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Teijin Multilon T-3011 Standard PC/ABS Polymer Alloy General grade of PC/ABS polymer alloy, having improved impact strength and heat resistance compared with a heat resistant ABS and flame retardant m-PPE and also having higher fluidity compared with .. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Styrolution Terblend® N NM-13 ABS/PA6 (Dry) Terblend N NM-13 is a new experimental ABS/PA6-Blend with improved impact strength at low temperatures. It can be easily processed on any standard injection molding machine.Information provided by .. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO Data |
Styron CALIBRE™ 200 15 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO Data |
Styron CALIBRE™ 2071 15 Polycarbonate, Sterilization Grade CALIBRE® 2071 resins are designed for those applications which use steam or ethylene oxide for sterilization while providing enhanced mold release characteristics. This material has excellent ret.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO Data |
Styron CALIBRE™ MEGARAD 2080 15 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | double V-notch, rk=1.5 mm; DIN 53753 |
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6) Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179-1 |
Total Lumicene® mPE M 3509 Medium Density Polyethylene, Blow Molding Lumicene® mPE M 3509 is a metallocene-based medium density polyethylene combining the features of conventional blow molding polyethylene with differentiated optical propertied such as gloss and co.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® L 25 NZ ESD PA12 Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of .. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 100ST BK602 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST BK602 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for Blow Molding Zytel LC6210 BK010 is a highly toughened heat stabilized polyamide 612 for extrusion blow molding or processing by other techniques requiring high .. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST801 is an unreinforced super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity r.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® 201-G0R PBT Resin Good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179 |
Teijin Multilon T-2711 Standard, Automobile Part Series PC/ABS Polymer Alloy PC/ABS polymer alloy general grade developed for automobile parts use. It has high heat resistance, impact strength, light resistance and fluidity, particularly, the high impact strength in a wide r.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | |
Akro-Plastic Akromid® A3 4 S1 PA, Cold-Impact Resistant
(discontinued **) The outstanding characteristic is the reduction of the normally common cooling brittleness at low temperatures. Here, AKROMID A has set a course with special combinations like high heat stabilizatio.. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | ISO 179-1 |
Unitika ET2025 PA6, Dry High-impact nylonInformation provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 8.00 J/cm² | 38.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Charpy Impact, Notched | 8.00 J/cm² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE8200 BK431 is an unreinforced, toughened, heat stabilized, lubricated high performance polyamide resin for injection molding. It is also a PPA resin.Information provided by DuPont Perfo.. |