Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Material ”S”® 1000 Green Polyethylene Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® Green Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from .. |
|||
Melting Point | 130 °C | 266 °F | |
Plastcom SLOVALEN PC 19 GF 20 PP, 20% glass fibre, mod. of mech. properties FeaturesModified copolymer PP for iextrusion, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. Applied i.. |
|||
Melting Point | 130 - 138 °C | 266 - 280 °F | ISO 3146 |
Polikim ULPOLEN® 500 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
Okulen® 500 PE-HMW, Coloured OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Melting Point | 130 °C | 266 °F | ASTM D3417 |
NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin Features: High ESCR, good toughness, good chemical resistance, good processability.Applications: Pipe coatings, profile extrusions, sheet extrusion for thermoforming, corrugated tubing, conduit.Data.. |
|||
Melting Point | 130 - 155 °C | 266 - 311 °F | Huntsman/TMA |
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melting Point | 130 °C | 266 °F | HS Method |
Hyosung Topilene C600H PP C600H Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Very low sealSlip propertyTransparencyInformation provided by Hyosung Corporation |
|||
Melting Point | 130 °C | 266 °F | |
Hyosung Topilene C600H2 PP C600H2 Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Melting Point | 130 - 131 °C | 266 - 268 °F | Crystalline MP |
Garland Manufacturing GAR-DUR® Ultra High Molecular Weight Polyethylene (UHMW-PE) GAR-DUR® plastic parts are made from ultra high molecular weight (UHMW) polymer having a molecular weight of 4.2 million and greater. Garland Manufacturing Company has been processing UHMW resin .. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC H1501 Polypropylene Homopolymer Features: SEETEC H1501 is a homopolymer for injection molding. H1501 is specifically developed for application demanding a high stiffness and a high fluidity. SEETEC H1501 meets the FDA requirement .. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC M1315 Polypropylene Impact Copolymer Features: SEETEC M1315 is a heterophasic polypropylene copolymer for compression molding caps, especially SACMI machines. SEETEC M1315 exhibits an excellent stiffness, a high impact strength, a high.. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC M1400 Polypropylene Impact Copolymer Features: SEETEC M1400 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1400 exhibits a high flowability and a good balance of stiffness and impact strength. SEE.. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC R3450 Polypropylene Random Copolymer Features: Seetec R3450 is a polypropylene-ethylene random copolymer designed for the production of cast films. It has a good clarity due to the optimum content of ethylene and offers optimum balance.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | Crystalline melting range |
Mikro-Technik Mikrolen UHMW-PE Properties: very good impact resistance / high absorption at shock and impact stress extremely high resistance against abrasive wear good corrosion resistance highly resistant at temperatures of -26.. |
|||
Melting Point | 130 - 140 °C | 266 - 284 °F | MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® 12C75 Thermoplastic Polyurethane Pearlbond® 12C75 is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low softe.. |
|||
Melting Point | 130 - 136 °C | 266 - 277 °F | DSC |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF) Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit.. |
|||
Melting Point | 130 °C | 266 °F | DSC |
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio.. |
|||
Melting Point | 130 °C | 266 °F | ASTM D-3418 |
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren.. |
|||
Melting Point | 130 °C | 266 °F | ASTM D-3418 |
Chevron Phillips Marlex® HMN TR-945/945G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationGood impact stren.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DIN 53 736 |
Hippe PE 500 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Melting Point | 130 °C | 266 °F | Dow Method (DSC) |
Dow DMDA-8920 NT 7 High Density Polyethylene Resin DOW DMDA-8920 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info.. |
|||
Melting Point | 130 °C | 266 °F | Dow Method (DSC) |
Dow DMDB-7950 NT 7 High Density Polyethylene Resin DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo.. |
|||
Melting Point | 130 °C | 266 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® CA 6 E PA* Product description: Grilon CA 6 E is a non-extracted copolyamide with a low melting point. Grilon CA 6 E characterizes itself through the following properties Very high flexibility and toughnessVer.. |
|||
Melting Point | 130 °C | 266 °F | ASTM D3418 |
ExxonMobil HD 6605.70 Injection Molding Resin Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan.. |
|||
Melting Point | 130 °C | 266 °F | ASTM D4591 |
3M Dyneon™ THVP 2030GZ Fluorothermoplastic Granules THVP 2030GZ is a very flexible, transparent fluoroplastic composed of fluorinated monomers. It is ideal for applications that require the good temperature, chemical and flame resistance of a fluorop.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
Okulen® 500 PE-HMW, Natural OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Melting Point | 130 - 136 °C | 266 - 277 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers. |