MBA Polymers PP 2131 F20 Post-consumer recycled polypropylene copolymer with approximately 20% fillers

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer MBA Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MBA Polymers PP 2131 F20 Post-consumer recycled polypropylene copolymer with approximately 20% fillers.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in standard black.Information provided by MBA Polymers.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
MBA Method
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa

@Temperature 23.0 °C
3480 psi

@Temperature 73.4 °F
ISO 527-2/50
Flexural Modulus 2.00 GPa

@Temperature 23.0 °C
290 ksi

@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Processing Properties Metric English Comments
Melt Temperature 180 - 210 °C
356 - 410 °F
Extrusion Range
200 °C
392 °F
Recommended Extrusion
200 °C
392 °F
Recommended Injection Molding
190 - 220 °C
374 - 428 °F
Injection Molding Range
Mold Temperature 40.0 °C
104 °F
Recommended
30.0 - 60.0 °C
86.0 - 140 °F
Drying Temperature 80.0 °C

@Time 3600 - 7200 sec
176 °F

@Time 1.00 - 2.00 hour
Moisture Content <= 0.10 %
<= 0.10 %