Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 50/CF/7/GS/10/TF/5/EM/BK Polycarbonate, with carbon fiber, glass flakes and PTFE, easy flowing

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Carbon Fiber Reinforced
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 50/CF/7/GS/10/TF/5/EM/BK Polycarbonate, with carbon fiber, glass flakes and PTFE, easy flowing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved friction and wear behaviour. Emergency running property.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance range.Body and duty parts in office equipment, gear wheels, grippers.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ISO 1183
Water Absorption <= 0.20 %
<= 0.20 %
23°C/24h
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Stress 90.0 MPa
13100 psi
Elongation at Yield 3.0 %
3.0 %
4.0 %
4.0 %
flexural
Modulus of Elasticity 6.00 GPa
870 ksi
Flexural Strength 130 MPa
18900 psi
Flexural Modulus 5.00 GPa
725 ksi
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
flatwise; ISO 179 1fU
2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179 1eA
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179 eA
Coefficient of Friction, Dynamic 0.26
0.26
Coefficient of Friction, Static 0.22
0.22
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C
25.0 µin/in-°F
DIN 53752
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 130 °C
266 °F
150 °C
302 °F
short term
Vicat Softening Point 160 °C
320 °F
DIN ISO 306
Flammability, UL94 V-1
V-1
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+7 ohm
<= 1.00e+7 ohm
Insulation Resistance <= 1.00e+7 ohm
<= 1.00e+7 ohm
Processing Properties Metric English Comments
Processing Temperature 295 °C
563 °F
mass temp
Nozzle Temperature 290 - 310 °C
554 - 590 °F
Zone 1 280 - 300 °C
536 - 572 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 300 - 320 °C
572 - 608 °F
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Drying Temperature 120 °C

@Time 14400 - 21600 sec
248 °F

@Time 4.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color black