Polymer Property : Zone 2 = 590 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-1109 Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7177 Polyamide 66, with PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7390 Polyamide 66, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8259 Polyamide 66, with glass fiber, thermally conductive modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Emergency running property.Coil formers, duty parts in plugs and switches, ..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8357 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Electrically conductive, suitable for continuous dischar..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8491 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50/CF/20 Polycarbonate, with carbon fiber, low-warpage
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50/TF/15/BK-1 Polycarbonate, with PTFE, easy flowing
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50-0789 Polycarbonate, with carbon fiber, easy flowing
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50-7164/BL02 Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Low warpag..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50-7807 Polycarbonate, with carbon fiber and demolding aid
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50-7844 Polycarbonate, with carbon fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts; low thermal coefficient of expansion.Redu..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50-8076 Polycarbonate, with carbon fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss ELECTRAFIL M-2386 Polycarbonate, with carbon fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/CF/10/GF/20/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/CF/20/HS Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/HS/BK Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Improved friction and wear behaviour. Emergency running propert..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-0867 Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinka..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-3260/schwarz Polyamide 66, with PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7360/EG Polyamide 66, with PTFE, lubricant modified, high viscosity, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property.Bea..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7943 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7956 Polyamide 66, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 50/GF/20/TF/20/BK 100 Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® G Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding ele..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® PA66/TF/40 Polyamide 66, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOTECH® GS 58 Polyamide 66, with glass fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/GF/20/TF/10/SI/2/BK Polyamide 66, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8130 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8228 Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 2 290 - 310 °C
554 - 590 °F
Lehmann & Voss PLASLUBE NY-1/SI/2/NT Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Information provided by Lehmann ..