Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.33 g/cc | 1.33 g/cc | Method A; ASTM D792 |
LNP Stat-Kon® LC-1003 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good Moldability, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® HFD4472 PC (Europe-Africa-Middle East) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
RTP Company RTP 203G HS Nylon 4/6 (PA 4/6) Glass Fiber 20% - Heat Stable
(discontinued **) Glass Fiber 20% - Heat StableComments:Glass FiberHeat Stable(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Infor.. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E818-10/23-CRM White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1502-7867/BL4 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ISO 1183 |
GEHR Plastics POM-ESD Acetal, Antistatic Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 822-10/148-CRB-LMP White PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
Spartech PETG 3D Lenticular 3-D Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | 23°C; ASTM D792 |
Teknor Apex MF 588 Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SIC 3710 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: High Impact ResistanceUses: Rigid Packing; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue LL40348/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® LL40348/4 is an aviation blue color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® LL40348/.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Red LL50304/3 Concentrate Based In LLDPE DescriptionPOLYBATCH® LL50304/2 is a red color concentrate based in LLDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL50304/2 is heavy .. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D 792 |
RTP Company RTP 2303 C Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D 792 |
RTP Company RTP 2502 FR Polycarbonate/ABS Alloy (PC/ABS), Glass Fiber - Flame Retardant - Non-PBBO/E - UL94 V-0 |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D 792 |
RTP Company RTP 203 C TFE 20 Nylon 11 (PA); Glass Fiber - PTFE Lubricated - 59% Renewable Resource Content Renewable Resource Content calculated based on % of total compound weight. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D 792 |
RTP Company RTP 2299 X 123311 A Polyetheretherketone (PEEK) Carbon Nanotube - ESD Protection |
|||
Specific Gravity | 1.33 g/cc @Temperature 25.0 °C |
1.33 g/cc @Temperature 77.0 °F |
|
Dow Corning 220 FLAKE RESIN Resin binder powder coating binder or co-binder to improve heat stability and weatherability; for blending with other silicone resins to reduce VOC content; in solvent-based organic coatings to impr.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
Colorite Polymers 8334 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
Colorite Polymers CS6033UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D-792 |
Axiall UV-6685 Rigid PVC, Molding Georgia Gulf UV 6685 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of parts requiring resistance to outdoor UV degradation.Info.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | |
Aremco Heat-Away™ 640 Thermally Conductive Grease, Copper Filled Aremco's Heat-Away™ thermal greases are ceramic and metal-filled silicone systems which offer exceptional thermal and electrical properties to 550 ºF. These materials are used in high-power electr.. |
|||
Specific Gravity | 1.33 - 1.37 g/cc | 1.33 - 1.37 g/cc | ASTM D-792 |
Axiall 16882 Coax & Telecom Flexible PVC Non-lead stabilized, 90C rated jacket compound with excellent low temperature properties. Formulated to be UV and fungal resistant. Suitable for riser and optical fiber constructions.Information p.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PX01658 PA 6 LNP* Thermocomp* PX01658 is a compound based on Nylon 6 containing Proprietary Fillers. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL CN5246 PPE+PS (Asia Pacific) |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SBB 3707 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Medium Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provi.. |
|||
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
RTP Company RTP 900 TFE 15 Z Polysulfone (PSU) PTFE 15% - FDA Type
(discontinued **) PTFE 15% - FDA TypeComments:PTFE LubricatedFDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by .. |