Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Maximum Moisture Content 0.010
0.010
Extrusion Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0070 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Yield 40.2 MPa

@Thickness 3.20 mm
5830 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break 35 %

@Thickness 3.20 mm
35 %

@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Yield >= 5.0 %

@Thickness 3.20 mm
>= 5.0 %

@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Yield Strength 66.7 MPa

@Thickness 3.20 mm
9670 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus 1.96 GPa

@Thickness 3.20 mm
284 ksi

@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched 3.43 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
6.43 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
4.22 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
7.90 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C

@Thickness 6.40 mm
203 °F

@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C

@Thickness 6.40 mm
185 °F

@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 95.0 °C

@Load 5.00 kg
203 °F

@Load 11.0 lb
50°C/h; ASTM D1525
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Zone 1 180 - 210 °C
356 - 410 °F
Extrusion Molding
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
Zone 3 200 - 250 °C
392 - 482 °F
Extrusion Molding
Zone 4 200 - 250 °C
392 - 482 °F
Extrusion Molding
Adapter Temperature 200 - 250 °C
392 - 482 °F
Extrusion Molding
Die Temperature 200 - 250 °C
392 - 482 °F
Extrusion Molding
Melt Temperature 200 - 250 °C
392 - 482 °F
Extrusion Molding
Roll Temperature 60.0 - 90.0 °C
140 - 194 °F
Bottom, Extrusion
70.0 - 90.0 °C
158 - 194 °F
Middle, Extrusion
70.0 - 100 °C
158 - 212 °F
Top, Extrusion
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Extrusion Molding
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Extrusion Molding