Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 66.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 66.7 MPa
9670 psi
ASTM D790
Samsung Cheil Industries Starex® SD-0150 ABS, Unreinforced  (discontinued **)
Amorphous Acrylonitrile Butadiene Styrene (ABS)Characteristics: General Purpose: Good Impact Strength, Chemical Resistance, ProcessabilityApplications: Household Appliances, Auto Interior Trim and P..
Flexural Yield Strength 66.7 MPa

@Thickness 6.40 mm
9670 psi

@Thickness 0.252 in
15 mm/min; ASTM D790
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow
Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information ..
Flexural Yield Strength 66.7 MPa

@Thickness 3.20 mm
9670 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 66.7 MPa

@Thickness 6.40 mm
9670 psi

@Thickness 0.252 in
15 mm/min; ASTM D790
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance
Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf..
Flexural Yield Strength 66.7 MPa

@Thickness 6.40 mm
9670 psi

@Thickness 0.252 in
15 mm/min; ASTM D790
LG Chemical AF308 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi..
Flexural Yield Strength 66.7 MPa

@Thickness 6.40 mm
9670 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Flexural Yield Strength 66.7 MPa

@Thickness 6.40 mm
9670 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade
High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali
Flexural Yield Strength 66.7 MPa

@Thickness 6.40 mm
9670 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron TIM 300 MMA- ABS
High Impact(Transparent ABS)Information provided by Bhansali
Flexural Yield Strength 66.7 MPa

@Thickness 6.40 mm
9670 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron KU-650 ABS Super Heat Resistant
High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali
Flexural Yield Strength 66.7 MPa

@Thickness 6.40 mm
9670 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Flexural Yield Strength 66.7 MPa

@Thickness 6.40 mm
9670 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade
High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali
Flexural Yield Strength 66.7 MPa

@Thickness 6.40 mm
9670 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron TIM 300 MMA- ABS
High Impact(Transparent ABS)Information provided by Bhansali
Flexural Yield Strength 66.7 MPa

@Thickness 6.40 mm
9670 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron KU-650 ABS Super Heat Resistant
High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali
Copyright © lookpolymers.com All Rights Reserved