Polymer Property : Izod Impact, Notched = 4.22 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.22 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
7.90 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HI100 ABS, High Impact
Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 4.22 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
7.90 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HI100H ABS, High Impact, High Toughness
Feature: Injection Molding, High Impact, High ToughnessApplication: Helmet, Pipe & Fittings)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 4.22 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
7.90 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 4.22 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
7.90 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical SH610A ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 4.22 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
7.90 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8010
Availability: North AmericaForms: PelletsProcessing Method: Extrusion Blow Molding and Sheet ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 4.22 J/cm

@Thickness 6.35 mm
7.90 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR
Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 4.22 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
7.90 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.22 J/cm

@Thickness 6.35 mm
7.90 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR
Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 4.22 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
7.90 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.