Polymer Property : Izod Impact, Notched = 3.43 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.43 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
6.43 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical MP211 ABS, Low Gloss, Metal Plating
Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical
Izod Impact, Notched 3.43 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
6.43 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane
Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 3.43 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
6.43 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 3.43 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
6.43 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 3.43 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
6.43 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.43 J/cm

@Thickness 3.17 mm
6.43 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade
Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 3.43 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
6.43 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 3.43 J/cm

@Thickness 3.17 mm
6.43 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade
Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 3.43 J/cm

@Temperature 0.000 °C
6.43 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SCG Chemicals EL-Leneâ„¢ H1000P High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Water pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals
Izod Impact, Notched 3.43 J/cm

@Temperature 23.0 °C
6.43 ft-lb/in

@Temperature 73.4 °F
ASTM D256
E-Polymers SEPAZ® LC50 PP Copolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.43 J/cm

@Temperature -30.0 °C
6.43 ft-lb/in

@Temperature -22.0 °F
ASTM D256
E-Polymers SEPAZ® LC50 PP Copolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.43 J/cm

@Thickness 6.40 mm
6.43 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade
Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali
Izod Impact, Notched 3.43 J/cm

@Temperature 23.0 °C
6.43 ft-lb/in

@Temperature 73.4 °F
ASTM D256
E-Polymers SEPAZ® LB50 PA6 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.43 J/cm

@Temperature -30.0 °C
6.43 ft-lb/in

@Temperature -22.0 °F
ASTM D256
E-Polymers SEPAZ® LB50 PA6 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.43 J/cm

@Temperature 23.0 °C
6.43 ft-lb/in

@Temperature 73.4 °F
ASTM D256
E-Polymers SEPAZ® LB60 PA6 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.43 J/cm

@Temperature -30.0 °C
6.43 ft-lb/in

@Temperature -22.0 °F
ASTM D256
E-Polymers SEPAZ® LB60 PA6 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 3.43 J/cm

@Thickness 6.40 mm
6.43 ft-lb/in

@Thickness 0.252 in
ASTM D256
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade
Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali