Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 200 °C | 392 °F | Zone 1 |
Premix Thermoplastics PRE-ELEC® CP 1315
(discontinued **) PRE-ELEC CP 1315 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Die Temperature | 200 °C | 392 °F | Zone 5 |
Premix Thermoplastics PRE-ELEC® CP 1316
(discontinued **) PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis.. |
|||
Die Temperature | 200 - 215 °C | 392 - 419 °F | Extrusion |
Huntsman IROGRAN® A 95 E 4861 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A95 4861 is a high performance polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN A95E 4861 is part of the HUNTSMAN technical extrusion pro.. |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS657 ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 200 - 210 °C | 392 - 410 °F | |
Lubrizol Advanced Materials PEARLTHANE® D16N98UV Thermoplastic Polyurethane Elastomer Pearlthane® D16N98UV is a polyether-based TPU, supplied in form of transparent, colorless pellets, combining high hardness with excellent mechanical properties and good hydrolysis and microbial r.. |
|||
Die Temperature | 200 °C | 392 °F | |
Taiwan PU Corporation TPU-B95 General Grade, Blow Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
Die Temperature | 200 °C | 392 °F | |
Taiwan PU Corporation TPU-BH95 Hydrolysis Resistance, Blow Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), Hydrolysis Resistance, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
Die Temperature | 200 °C | 392 °F | |
Taiwan PU Corporation TPUI-E95 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Die Temperature | 200 °C | 392 °F | |
Taiwan PU Corporation TPUI-G90 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Die Temperature | 200 °C | 392 °F | |
Taiwan PU Corporation TPUI-H95 High Hydrolysis Resistance, Injection Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Die Temperature | 200 °C | 392 °F | Body |
SK Chemicals SKYTHANE® S190A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Die Temperature | 200 °C | 392 °F | Tip |
SK Chemicals SKYTHANE® S395A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Die Temperature | 200 °C | 392 °F | Tip |
SK Chemicals SKYTHANE® S398A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Die Temperature | 200 °C | 392 °F | Body |
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Die Temperature | 200 - 230 °C | 392 - 446 °F | |
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection BB412E is a natural, medium molecular weight, medium melt flow rate polypropylene block copolymer with an optimal mechanical properties balance resulting in high stiffness and very good impact stren.. |
|||
Die Temperature | 200 - 230 °C | 392 - 446 °F | |
Borealis BE50-7032 Polypropylene Homopolymer for Non-Pressure pipes and extruded sheets BE50-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer characterized by high stiffness, high heat distortion temperature and high resistance to thermal aging.
The materia.. |
|||
Die Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® HE3494-LS Dark Blue High Density Polyethylene for Drinking Water Pipes Borstar HE3494-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combina.. |
|||
Die Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® ME3441 Yellow Medium Density Polyethylene for Natural Gas Pipes Borstar ME3441 is a yellow, bimodal, cadmium free, medium density polyethylene compound classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. It includes a combinat.. |
|||
Die Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Die Temperature | 200 °C @Pressure 4.80 - 17.0 MPa |
392 °F @Pressure 696 - 2470 psi |
Extrusion |
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Die Temperature | 200 °C | 392 °F | Extrusion |
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Die Temperature | 200 °C @Pressure 4.80 - 17.0 MPa |
392 °F @Pressure 696 - 2470 psi |
Extrusion |
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Die Temperature | 200 °C @Pressure 4.80 - 17.0 MPa |
392 °F @Pressure 696 - 2470 psi |
Extrusion |
Alliance Polymers Viprene™ P70A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Die Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Die Temperature | 200 - 210 °C | 392 - 410 °F | |
Borealis Borstar® HE3490-LS Black High Density Polyethylene for Pressure Pipes Borstar HE3490-LS is a black, bimodal, high density polyethylene classified as an MRS 10.0 material (PE100) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding.. |