Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Resirene Resirene® HH-103 General Purpose Polystyrene Features:Low FlowHigh HeatHigh Molecular WeightMechanical StrengthFDA Rating: 21 CFR 177.1640Applications:ExtrusionFoamGPPS/HIPS BlendsInformation provided by US distributor Calsak Corporation. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | |
Mapal Plastics Maplon PAPER MATCH Polypropylene Sheet Paper match is a multi layer graphic sheet. The core layer is a high rigidity PP. The skin layers are high field polyolefine. The surface bonds easily to inks and have some absorbing capacity.Main a.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
LG Chemical LG703W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Specific Gravity | 1.04 - 1.06 g/cc | 1.04 - 1.06 g/cc | |
Michelman® SofTak® 317 Non-skid coating Description: Non-skid coating.Usage: SofTak® 317 is a gluable nonskid coating with excellent angle of skid. These properties are useful for slip or tier sheets, or a variety of other applications.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | |
Momentive Performance Materials RTV160 Electronic Grade Silicone Adhesive Sealant, White RTV160, RTV162, and RTV 167 adhesive sealants for GE silicones are one-component, ready-to-use electronic grade silicone sealants. They cure to a tough, resilient silicone rubber on exposure to atm.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Lucent Polymers ABS-305 Acrylonitrile Butadiene Styrene, General Purpose Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | |
Momentive Performance Materials RTV6702 One-Component, Modified Alkoxy Adhesive Sealant, White RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP MX06403 PP LNP* THERMOCOMP* MX06403 is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Supreme Petrochem SC 203 LV General Purpose Polystyrene CharacteristicsGood flow grade with good mechanical properties Good clarity and flexibility Easy processing grade and suitable for thin walled applicationsProcessing Extrusion MoldingApplicationsSu.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Supreme Petrochem SP 6410 0003 Abrasion Resistant Polystyrene Characteristics Self lubricating, abrasion resistant Low specific Gravity Suitable for multicavity thin wall parts Excellent thermal stability and easy to color Processing Injection moldingApplic.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Supreme Petrochem SP6432 9690 Medium Impact Polystyrene Characteristics High flow Good toughness Available in various colors Processing Injection moldingApplications Air conditioner and cooler grills Refrigerator parts Washing machine components Mate.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL PX0888 PPE+PS Unfilled, non-FR. Higher heat resistance than N110 (BOZ) and px0844 (USA). For automotive interiors. 250F (121C) DTUL. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
ELASTO UK Dryflex® 420401S SBS Based Material, 40D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Diamond Polymers ABS 4012B Blow Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Entec Hyrene® PS-HI 3/3 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8271-55B100 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Diamond Polymers GPPS BEADS Injection Molding Grade, General Purpose Polystyrene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Americas Styrenics EA3130 High Heat Crystal Polystyrene Product CharacteristicsAdditive FreeFood Contact CompliantTypical ApplicationsMedical PartsColor Concentrate CarrierLow Profile AdditivesInformation provided by AmericasStyrenics LLC. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | Laminate; ASTM D792 |
Azdel Plus C220-B01 22% Chopped Fiber Mat / PP Resin Matrix AZDEL® C220-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Americas Styrenics STYRON® 695 High Heat Crystal Polystyrene Product CharacteristicsReduced residualsHigh heat resistancehigh strengthFood Contact CompliantTypical ApplicationsOPSInformation provided by AmericasStyrenics LLC. |
|||
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ISO 2782 |
AlphaGary Evoprene™ GC 5658 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |