Ineos HP53-25-155 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos HP53-25-155 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HP53-25-155 is a high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blow molding equipment, specifically where applications which require excellent environmental stress crack resistance (ESCR). This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D4883
Melt Flow 0.22 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.22 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Yield 25.5 MPa
3700 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break >= 700 %
>= 700 %
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 0.931 GPa
135 ksi
2% Secant-Method 1; ASTM D790
1.138 GPa
165.1 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 1.70 J/cm
3.18 ft-lb/in
ASTM D256
Tensile Impact Strength 313 kJ/m²
149 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C
160 °F
ASTM D648
Vicat Softening Point 129 °C
264 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Blow Molding
Region US & Canada