Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | |
Eastman Eastar GN101 PETG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
ExxonMobil HD 6908.18 Injection Molding Resin
(discontinued **) HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requiring very high stif.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
LyondellBasell Alathon® M6028 High Density Polyethylene ApplicationsM 6028 is a homopolymer that is warp resistant, exhibits excellent toughness, stiffness and color as well as low odor and good processing stability. Typical applications include safety .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
Ineos Barex® 218 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 218E is most commonly used for thermoformed sheet applications in which high impact performance is require.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
Ineos HP53-25-155 HDPE HP53-25-155 is a high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blow molding equipment, specifically where appli.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C @Thickness 3.20 mm |
160 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C @Thickness 3.20 mm |
160 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR (Asia Pacific) LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | Unannealed; ASTM D648 |
Lubrizol Isoplast® 2510 Engineering Thermoplastic Polyurethane Resin Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ISO 75-2 |
Borealis MG7547B Polyethylene MG7547B is a high-density polyethylene produced by a low pressure process. This grade has an excellent impact strength and low distortion even at low temperatures. It also contains UV stabilizer, wh.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ISO 75-2 |
Borealis MG7547S Polyethylene MG7547S is a high-density polyethylene produced by a low pressure process. This grade has an excellent impact strength and low distortion even at low temperatures. It also contains UV stabilizer, wh.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | Unannealed; ASTM D648 |
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
Eastman Cadence™ GS2 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
Eastman Eastar CN005 Copolyester, High Flow Grade Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
Eastman Eastar CN015 Copolyester, High Flow Grade with Mold Release Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
Eastman Eastar EN063 Polyester Eastar Polyester EN063 is a condensation polymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Eastar Polyester EN063 is a homopolymer .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
Entec Hypro™ PP-CP35/1.5C Impact Copolymer, 35 Melt Flow This product is intended for general purpose injection molding applications especially those requiring fast cycle time, improved color, enhanced processability, and excellent clarity.Information pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | Unannealed; ASTM Data |
Dow Prevail® 3100 ABS + Polyurethane PREVAIL® 3100 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM-D648 |
Braskem GP100BK HDPE High Density Extrusion Polyethylene GP100BK is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for water distribution. It is produced with bimodal technology and has high molar mass. It.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM-D648 |
Braskem GP5550 HDPE High Density Extrusion Polyethylene GP5550 is a high-density polyethylene with high molar mass. It is produced with bimodal technology and shows excellent mechanical properties and high resistance to stress cracking. Its applications .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM-D648 |
Braskem GP5550BK HDPE High Density Extrusion Polyethylene GP5550BK is a high-density polyethylene with high molar mass. It is produced with bimodal technology and shows excellent mechanical properties and high resistance to stress cracking. GP5550BK contai.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
Braskem JV 060U HDPE Injection Molding Polyethylene Applications: Caps, crates for industrial, transportation or fishing uses, industrial pails, stands and pallets, refuse containers; bottle cases, safety helmets, cages for poultry transportation and.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM-D648 |
Braskem BS002HS HDPE Blow Molding Polyethylene Copolymer Resin BS002HS is a high-density polyethylene, bimodal copolymer. It presents good rigidity, good impact resistance, and good reproducibility of the weight of the bottles. It also has excellent envir.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM-D648 |
Braskem IG58 HDPE Injection Molding Polyethylene Copolymer IG58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high stiffness, impact strength and out.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
Braskem JV060U Injection Molding High Density Polyethylene Boxes for beverages bottles; Boxes in general; Technical parts.Information provided by Braskem. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ISO 75-2 |
Borealis MG9601 Polyethylene MG9601 is a natural high-density polyethylene with high melt-index and narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. The grade is characterized by exce.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM D648 |
Ineos HP50-25-153 HDPE A high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which requiring excellent environmental stress crack resistance (ESCR)... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 71.0 °C | 160 °F | ASTM-D648 |
Braskem BS600 HDPE Blow Molding Polyethylene Copolymer BS600 resin is a high-density polyethylene (HDPE), bimodal copolymer offering an outstanding combination of impact resistance and environmental stress crack resistance (ESCR). It is thus recommended.. |