Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 1.138 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.138 - 1.793 GPa
165.1 - 260.1 ksi
ASTM D790
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Flexural Modulus 1.138 GPa
165.1 ksi
ASTM D790
Flint Hills PP 13T10A cs279 Random Copolymer Polypropylene
Random copolymer with antistat, clarified, and FDA compliant.Features: Excellent clarity, non-blushing, good impact resistance, and high stiffness.Applications: Injection molding: lab ware, food pac..
Flexural Modulus 1.138 GPa
165.1 ksi
Tangent-Method 1; ASTM D790
Ineos HP53-25-155 HDPE
HP53-25-155 is a high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blow molding equipment, specifically where appli..
Flexural Modulus 1.138 GPa
165.1 ksi
Tangent-Method 1; ASTM D790
Ineos K50-10-136 HDPE
Ineos K50-10-136 is a high molecular weight, high density polyethylene copolymer. This product was developed for blowmolding automotive fuel tanks and other large parts, where the finished produc..
Flexural Modulus 1.138 GPa
165.1 ksi
3 pt. secant. ASTM D790
Chevron Phillips HiD® 9512/HiD® 9513 with Antistat HDPE Blow Molding Resin  (discontinued **)
Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo..
Flexural Modulus 1.138 - 2.07 GPa
165.1 - 300 ksi
ASTM D790
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Flexural Modulus 1.138 GPa
165.1 ksi
Tangent-Method 1; ASTM D790
Ineos HP50-25-153 HDPE
A high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which requiring excellent environmental stress crack resistance (ESCR)...