Dow Corning 9546 Silicone Elastomer Blend

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 9546 Silicone Elastomer Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane and a high molecular weight linear silicone polymer for use in skincare, suncare, shower gel, color cosmetic, hair care, and antiperspirant / deodorant applications.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity 250000 - 450000 cP
250000 - 450000 cP
Dynamic
Descriptive Properties Value Comments
Cyclotetrasiloxane Content (%) <1
Nonvolatile Content (%) 15-16