Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.22 g/10 min | 0.22 g/10 min | I<sub>2</sub>; ASTM D1238 |
Petromont 4101 High Density Polyethylene Resin Petromont HDPE 4101 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is primarily used in the extrusion of corrugated pipes for drainage applications, f.. |
|||
Melt Flow | 0.22 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos HP53-25-155 HDPE HP53-25-155 is a high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blow molding equipment, specifically where appli.. |
|||
Melt Flow | 0.22 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos HP55-25-155 HDPE A high performance high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blowmolding equipment, specifically where applications require ex.. |
|||
Melt Flow | 0.22 g/10 min | 0.22 g/10 min | |
JPJ Technologies 6360M HDPE Extrusion Information provided by JPJ Technologies |
|||
Melt Flow | 0.22 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.22 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
SCG Chemicals EL-Leneâ„¢ H1000P High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Water pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals |
|||
Melt Flow | 0.22 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE AA48-002 High Density Polyethylene Resin Product Description: AA48-002 is a blow molding grade high density polyethylene copolymer containing an antistatic additive. It provides a very good balance of stress crack resistance, stiffness and.. |
|||
Melt Flow | 0.22 g/10 min @Load 2.16 kg |
0.22 g/10 min @Load 4.76 lb |
|
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade DOW LDPE 133A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of antib.. |
|||
Melt Flow | 0.22 g/10 min @Load 2.16 kg |
0.22 g/10 min @Load 4.76 lb |
|
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade DOW LDPE 135A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of slip .. |
|||
Melt Flow | 0.22 g/10 min @Load 2.16 kg |
0.22 g/10 min @Load 4.76 lb |
|
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade DOW LDPE 132I is a barefoot resin for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It complies with U.S. FDA re.. |
|||
Melt Flow | 0.22 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.22 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GP100BK HDPE High Density Extrusion Polyethylene GP100BK is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for water distribution. It is produced with bimodal technology and has high molar mass. It.. |
|||
Melt Flow | 0.22 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.22 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GP100OR HDPE High Density Extrusion Polyethylene GP100OR is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal technology and has high molar mass. It s.. |
|||
Melt Flow | 0.22 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.22 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos HP50-25-153 HDPE A high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which requiring excellent environmental stress crack resistance (ESCR)... |