Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.138 - 1.793 GPa | 165.1 - 260.1 ksi | ASTM D790 |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Flexural Modulus | 1.138 GPa | 165.1 ksi | ASTM D790 |
Flint Hills PP 13T10A cs279 Random Copolymer Polypropylene Random copolymer with antistat, clarified, and FDA compliant.Features: Excellent clarity, non-blushing, good impact resistance, and high stiffness.Applications: Injection molding: lab ware, food pac.. |
|||
Flexural Modulus | 1.138 GPa | 165.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos HP53-25-155 HDPE HP53-25-155 is a high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blow molding equipment, specifically where appli.. |
|||
Flexural Modulus | 1.138 GPa | 165.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos K50-10-136 HDPE Ineos K50-10-136 is a high molecular weight, high density polyethylene copolymer. This product was developed for blowmolding automotive fuel tanks and other large parts, where the finished produc.. |
|||
Flexural Modulus | 1.138 GPa | 165.1 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9512/HiD® 9513 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Flexural Modulus | 1.138 - 2.07 GPa | 165.1 - 300 ksi | ASTM D790 |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Flexural Modulus | 1.138 GPa | 165.1 ksi | Tangent-Method 1; ASTM D790 |
Ineos HP50-25-153 HDPE A high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which requiring excellent environmental stress crack resistance (ESCR)... |