DuPont™ Bynel® 41E865 Anhydride Modified LLDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer DuPont
Trade Name Bynel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Bynel® 41E865 Anhydride Modified LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins. Physical properties of BYNEL Series 4100 resins are typical of linear low-density polyethylene resins with similar density and melt index values. Use of these adhesive resins in coextruded PE/barrier structures offers improved thermal resistance over that of ethylene vinyl acetate-based adhesive resins. BYNEL 4100 series resins adhere to a variety of materials. They are most often used to adhere to EVOH, polyamide, PE and ethylene copolymers. BYNEL 41E865 is also known for its ability to adhere to PS (polystyrene) in the coextrusion process. Series 4100 resins can be used in coextrusion processes including: blown film cast film/sheet blow molding melt and solid phase thermoforming sheet and tubing LLDPE resins are known for their temperature resistance and toughness. These physical properties make the 4100 series resins work well in applications such as: boil-in-bag structures blow molded containers in which drop strength is important bag-in-box films film where LLDPE is the heat seal layer. BYNEL 41E865 resin conforms with the Code of Federal Regulations, Title 21, Paragraph 175.105, covering the use of adhesive interlayers in composite packages for food use. This regulation describes adhesives that may be safely used as components of articles intended for use in packaging, transporting or holding food. This regulation requires that either (1) the adhesive is separated from the food by a functional barrier, or (2) the quantity of adhesive which contacts fatty or aqueous foods does not exceed the trace amounts at the seams or edges. Customers should satisfy themselves that the food contact material is serving as a functional barrier to the adhesive.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792, ISO 1183
Melt Flow 4.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 106 °C
223 °F
Freezing Point; ASTM D3418
109 °C
228 °F
ASTM D3418, ISO 3146
Vicat Softening Point 82.0 °C
180 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 250 °C
<= 482 °F
Feed Temperature 160 °C
320 °F
CoExtrusion with EVOH Processing
160 °C
320 °F
CoExtrusion with Nylon Processing
Zone 2 185 °C
365 °F
CoExtrusion with EVOH Processing
185 °C
365 °F
CoExtrusion with Nylon Processing
Zone 3 235 °C
455 °F
CoExtrusion with EVOH Processing
235 °C
455 °F
CoExtrusion with Nylon Processing
Zone 4 235 °C
455 °F
CoExtrusion with EVOH Processing
250 °C
482 °F
CoExtrusion with Nylon Processing
Zone 5 235 °C
455 °F
CoExtrusion with EVOH Processing
250 °C
482 °F
CoExtrusion with Nylon Processing
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
250 °C
482 °F
CoExtrusion with Nylon Processing
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
250 °C
482 °F
CoExtrusion with Nylon Processing
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
<= 250 °C
<= 482 °F
CoExtrusion with Nylon Processing