Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
Plaskolite PETG Mirror Sheet Versatile fabrication properties with good impact strength, good design flexibility, and speed of fabrication.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific) Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied.. |
|||
Vicat Softening Point | 82.0 °C @Load 1.00 kg |
180 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® MT 10 R Low Density Polyethylene - Injection Molding Riblene MT 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 R are highly flexible.Main Applications: Riblene MT 10 R is suitable for inject.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | DIN 53460 |
Polycasa PETG QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits o.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
DuPont Bynel® 3095 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 241 Rigid PVC, Extrusion Various profiles |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 425 Rigid PVC, Extrusion Electric channels |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 425/R Rigid PVC, Extrusion Shiny electric channels |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5053 500 Micron LDPE Powder Description: ICOFLO 510-5053 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5054 800 Micron LDPE Powder Description: ICOFLO 510-5054 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306B |
Lucite International Diakon® ST45G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306 |
Iran Petrochemical (PCC) 1922T Low Density Polyethylene LDPE 1922T - for injection molding with a balance between flow properties and mechanical propertiesApplications: toys, household articles, clamping lids.Information provided by Iran Petrochemical Co.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306 |
Stir SpA HE 63/1 (PVC) Application: Economic profile for good fluidityInformation provided by STIR SpA |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306 |
Stir SpA RTC PM A (PVC) Application: Shock resistant moldingInformation provided by STIR SpA |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 180A R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 3135XZ Ethylene Vinyl Acetate DuPont™ Elvax® 3135XZ is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Applicati.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306 |
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
Lubrizol Estane® R180A Thermoplastic Polyurethane Type: Estane® R180A is a Shore 83A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds R 218 Rigid PVC, Extrusion Shutters and shiny profiles |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds R 316 Rigid PVC, Extrusion Rolling shutters |
|||
Vicat Softening Point | 82.0 °C @Load 1.02 kg |
180 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem IP2418 LDPE Injection Molding Polyethylene IP2418 is a low-density polyethylene with good processability and high fluidity, flexibility, and mechanical strength. It does not contain additives. Its applications include injection molding and b.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | 50°C/hr; 50N |
Polimeri Europa EDISTIR SRL550 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,E,083-12-07-18 High impact, easy flow polystyrene with good elasticity at low temperatures. Used for sheet extrusion and .. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total Lacqrene® 6631 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 140/1 Rigid PVC, Extrusion Drain-pipes |
|||
Vicat Softening Point | 82.0 - 115 °C | 180 - 239 °F | Average value: 102 °C Grade Count:122 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 760Q Ethylene Vinyl Acetate DuPont™ Elvax® 760W is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 760Q resins can be used for the following applicati.. |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 230/D Rigid PVC, Extrusion Electric channels |