Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Nylex™ 1404 NAT Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing.. |
|||
Melt Flow | 4.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Nylex™ 2185 HFX Natural Polyamide + PP Forms: PelletsProcessing Methods:Injection moldingFeatures:Tensile Strength, HighInformation provided by Multibase |
|||
Melt Flow | 4.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Nylex™ 2185 NAT Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing.. |
|||
Melt Flow | 4.7 g/10 min | 4.7 g/10 min | ASTM D1238 |
LyondellBasell Microthene® F FN51000 Low Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Melt Flow | 4.7 g/10 min | 4.7 g/10 min | ASTM D1238 |
LyondellBasell Microthene® F FN51900 Low Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Melt Flow | 4.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H05A-00 Polypropylene Homopolymer Grade H05A-00 is an antistatic polypropylene homopolymer for injection molding & extrusion applications. This material meeets the requirements of the U.S. Food and Drug Administration as specified .. |
|||
Melt Flow | 4.7 g/10 min | 4.7 g/10 min | ISO 1133 |
Iran Petrochemical (PCC) 2404TC47 Low Density Polyethylene LDPE 2404TC47 Light duty FilmIt is used for very thin films requiring good optical properties for general packaging applications e.g. covering film with very low blocking tendency.Information provi.. |
|||
Melt Flow | 4.7 g/10 min | 4.7 g/10 min | ISO 1133 |
Iran Petrochemical (PCC) 2004TC37 Low Density Polyethylene LDPE 2004TC37: Light duty film used for very thin films requiring good optical properties for general packaging.Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 4.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene LT0470/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. Application: stiffer thin films for textile p.. |
|||
Melt Flow | 4.7 g/10 min @Load 10.0 kg, Temperature 250 °C |
4.7 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL SE1 PPE+HIPS (Asia Pacific) PPE+HIPS Unfilled FR V-1 125C |
|||
Melt Flow | 4.7 g/10 min @Load 10.0 kg, Temperature 250 °C |
4.7 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL SE1V PPE+HIPS (Asia Pacific) PPE/HIPS, unfilled, FR-V1, 90 oC |
|||
Melt Flow | 4.7 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.7 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styron Magnumâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines ex.. |
|||
Melt Flow | 4.7 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.7 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styron MAGNUMâ„¢ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology of Styron ensures an ABS tech.. |
|||
Melt Flow | 4.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Melt Flow | 4.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Melt Flow | 4.7 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.7 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers Centrex® 885 Profile Extrusion Grade Centrex 885 resin is a low-gloss ASA (acrylonitrile-styrene-acrylate) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can be coextruded over polyviny.. |
|||
Melt Flow | 4.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 1040 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 4.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 1102 K Polypropylene Grade with high processing stability for film tape (low water carryover), fibrillated film, monofilaments, OPP film (special formulations) and thermoformed parts.Data was collected by ISO methods an.. |
|||
Melt Flow | 4.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 2440 K Polypropylene Data was collected by ISO methods and provided by BASF. |