Polymer Property : Zone 3 = 235 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 1462Z PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 1462Z is a general purpose, 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.30% glass-fiber, general purposeInformation provid..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 1602Z PBT  (Unverified Data**)
Celanex 1602Z is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1602Z has an internal lubricant.Lubricated extrus..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3316 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3400-2 PBT, 40% Glass Reinforced  (Unverified Data**)
Celanex 3400-2 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 4302LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance, that is also enhanced for improved laser marking graphics.30% glass fiber, impact ..
Zone 3 235 - 255 °C
455 - 491 °F
Celanese Celanex® 5300-2 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 5300-2 is a 30% fiberglass reinforced polyester with improved surface finish. Celanex 5300-2 contains an internal lubricant.30% glass reinforced, high gloss, general purpose, lubricatedInfor..
Zone 3 235 - 255 °C
455 - 491 °F
Celanese Celanex® 6400-2 PBT, Mineral / Glass Reinforced  (Unverified Data**)
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.40% glass/mineral filled, low warpInformation provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Vandar® 4602Z PBT  (Unverified Data**)
4602Z is an unfilled thermoplastic alloy with good weatherability and chemical resistance.Unreinforced, good chemical resistanceInformation provided by Celanese
Zone 3 235 °C
455 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail..
Zone 3 235 °C
455 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE
BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru..
Zone 3 235 °C
455 °F
Extrusion Coating
DuPont™ Appeel® 20D784 Ethylene Acrylate
Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature ..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 1400FC PBT, Unfilled
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 2004-2 PBT, Unfilled
Celanex 2004-2 is an unfilled polyester that has an excellent combination of flowability and toughness. A typical application for Celanex 2004-2 is electrical connectors containing latches. Celanex ..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 2008 PBT, Unfilled
Celanex 2008 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by ..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 2401 MT PBT, Medical Technology
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3216HR PBT, 15% Glass Reinforced
Celanex 3216HR is a flame retarded, hydrolysis resistant, 15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability.Information ..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3300LM PBT, 30% Glass Reinforced
Celanex 3300LM is a 30% glass reinforced lasermarkable grade specially formulated to yield crisp marks when subjected to a Nd:YAG laser or equivalent operated at 1064nm or 532nm. Lasers operating i..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 4300FC PBT, 30% Glass Reinforced
Celanex 4300FC is a toughened, 30% glass reinforced PBT for use in food contact applications.Information provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 4309AR PBT
Celanex 4309AR is a 30% glass reinforced PBT with enhanced resistance to hydrolysis, alkaline environments and salt water spray.Information provided by Celanese
Zone 3 235 - 255 °C
455 - 491 °F
Celanese CELANEX 5200-2 PBT, 15% Glass Reinforced
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.Information provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 2003-2 PBT, Unfilled
Celanex 2003-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability, and good flow characterictics. Celanex 2003-2 is a medium h..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3201 PBT, 15% Glass Reinforced
Celanex 3201 is a 15% glass reinforced general purpose thermoplastic polyester resin that offers a superior combination of mechanical, electrical, and thermal properties, together with outstanding p..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityTo avoid hydrolytic degradation during processi..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese VANDAR 4612R PBT, 7% Glass Reinforced
Vandar 4612R is a high impact polyester alloy containing 7% glass. It possesses excellent impact properties as well as toughness and moldability. Dimensional stability, chemical resistance, and low ..
Zone 3 235 - 255 °C
455 - 491 °F
Celanese CELANEX 6500 PBT, 30% Mineral / Glass Reinforced
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability.Information provided by Celanese
Zone 3 235 - 255 °C
455 - 491 °F
Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced
Celanex 6406 is a 40% mineral/glass reinforced resin providing excellent toughness combined with warpage resistance, surface gloss and good mechanical properties. Celanex 6406 is particularly suited..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 2000-3FC PBT  (Unverified Data**)
Celanex 2000-3FC is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity for use in food contact applications.. Celanex 2000-3FC is a high flow mater..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese VANDAR 2122 PBT, 10% Mineral Reinforced
Vandar 2122 is a polyester alloy which contains 10% mineral filler. It offers exceptional toughness and practical impact strength. This resin offers Class A paintable finish with excellent dimension..