Thermal Properties Metric English Comments
Melting Point 106 - 116 °C
223 - 241 °F
Oceanchem Group Bis (2,3-dibromopropyl ether) of TBBA (BDDP)
Molecular Formula: C21H20Br8O2Cas No.: 21850-44-2Application: BDDP used for plastics as flame-retardant, is designed for use in PP (homopolymer and copolymer) and high impact polystyrene (HIPS) appl..
Melting Point 106 °C
223 °F
Internal method
Polimeri Europa Riblene® MT 10 Low Density Polyethylene - Injection Molding
Riblene MT 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 are highly flexible.Main Applications: Riblene MT 10 is suitable for injection mo..
Melting Point 106 °C
223 °F
Internal method
Polimeri Europa Riblene® MT 10 R Low Density Polyethylene - Injection Molding
Riblene MT 10 R is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MT 10 R are highly flexible.Main Applications: Riblene MT 10 R is suitable for inject..
Melting Point 106 °C
223 °F
Exxon Method
ExxonMobil Escorene® LD-144 EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 2% vinyl acetate copolymer packaging film resin. Film made from LD-144 offers improved impact strength and heat sealability compared to homopolym..
Melting Point 106 °C
223 °F
Exxon Method
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera..
Melting Point 106 °C
223 °F
Exxon Method
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit ..
Melting Point 106 °C
223 °F
DSC
LyondellBasell DP 8510M Polybutene
Key Features: semi-crystalline high ethylene content random copolymer, miscible with polyproylenesApplications: Hot Melt Adhesives, FDA acceptableMeets FDA requirements in 21 CFR 175.105 for indirec..
Melting Point 106 °C
223 °F
Melting point via DSC/ASTM D3418
DuPont Bynel® 4206 Anhydride-Modified LDPE Adhesive Resin
Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process ..
Melting Point 106 °C
223 °F
Melting point via DSC/ASTM D3418
DuPont Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin
Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process ..
Melting Point 106 °C
223 °F
ISO 11357
Total LDPE 1200 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
LDPE 1200 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: flexible molding, handles, closures, household items, toys, variou..
Melting Point 106 °C
223 °F
DSC; ASTM D3418
Westlake Tymax™ GT1057 Anhydride Modified Acrylate Copolymer
Product Description: Westlake GT1057 is an anhydride modified low density polyethylene designed as an extrusion coating and laminating tie-layer. Westlake GT1057 provides excellent adhesion to pol..
Melting Point 106 °C
223 °F
ASTM D1525
Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane
Features: High stiffness TPU alloyUses: Flat Die/Cast Sheet Extrusion, Profile Extrusion and Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided b..
Melting Point 106 °C
223 °F
Freezing Point; ASTM D3418
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Melting Point 106 °C
223 °F
Freezing Point; ASTM D3418
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Melting Point 106 °C
223 °F
Freezing Point; ASTM D3418
DuPont™ Fusabond® E589 Polymer Modifier
DuPont™ Fusabond® E589 is an anhydride modified polyethylene. Uses: Adhesives Pipe Coating Tie-Layer Features premium adhesive for Pipe Coating tie-layer at high surface temperatures. ( 90°C)
Melting Point 106 °C
223 °F
Dow Method (DSC)
Dow 4010 Low Density Polyethylene (LDPE)
Polyethylene 4010 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry and moist foods packaging, sugar pouches, lidding stoc..
Melting Point 106 °C
223 °F
DSC
Arkema Group OREVAC® 18921A Epoxide Modified Polyethylene
OREVAC® 18921A is epoxide modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 18..
Melting Point 106 °C
223 °F
ISO 11357-3
Addcomp PRIEX® 15005 Maleic Anhydride modified LDPE
Functionalised low density polyethylene to be used as compatibiliser for polymer blends or coupling agent for wood flour, natural fibres, or mineral filled polyolefins. Also suitable to reduce pigme..
Melting Point 106 °C
223 °F
BASF N,N’-Dimethylurea
Formula: C3H8N2OCAS: 96-31-1Description Dimethylurea is a colorless to white powder, with an amine-like odor.Synonyms: 1,3-DimethylureaApplications: Intermediate used in the production of Pharmaceut..
Melting Point 106 °C
223 °F
DSC
Arkema Group LOTADER® AX 8840 Copolymer Ethylene - Glycidyl Methacrylate
LOTADER AX 8840 is a random copolymer of Ethylene and Glycidyl Methacrylate, polymerized under high pressure in an autoclave process. Due to the reactivity induced by the Glycidyl methacrylate, LOTA..
Melting Point 106 °C
223 °F
ASTM D3417
DuPont Elvax® PE3507-2 Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® PE3507-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Applic..