Processing Properties Metric English Comments
Melt Temperature 200 - 235 °C
392 - 455 °F
SABIC F00952EQ High Density Polyethylene for Blown Film
Product Description: F00952EQ is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. the design of the product, molecular architect..
Melt Temperature 200 - 235 °C
392 - 455 °F
SABIC F04660 High Density Polyethylene for Blown Film Applications
Product Description: F04660 is a homopolymer HDPE film grade with excellent processability and high stiffness. It has good moisture barrier properties and can be blended with LDPE and LLDPE to imp..
Melt Temperature 200 - 235 °C
392 - 455 °F
SABIC FJ00952 High Density Polyethylene for Blown Film
Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, ..
Melt Temperature 179 - 235 °C
354 - 455 °F
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE)
Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p..
Melt Temperature 220 - 235 °C
428 - 455 °F
Extrusion
DuPont Performance Polymers Hytrel® 5553FG NC010 TPC-ET  (Unverified Data**)
Hytrel® 5553FG NC010 is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont
Melt Temperature 165 - 235 °C
329 - 455 °F
M. Holland Company MAGMA® Magmalene Polyalphaolefin  (discontinued **)
High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessUses: BlendingProcessing Method: Injection MoldingInformation provided by M. Holland.
Melt Temperature 205 - 235 °C
401 - 455 °F
Injection Molding
LG Chemical KEYFLEX BT 1245D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Medium Modulus, Black colorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical
Melt Temperature 220 - 235 °C
428 - 455 °F
Recommended for Injection
Kolon DIAMAT® GP
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Melt Temperature 220 - 235 °C
428 - 455 °F
Recommended for Injection
Kolon DIAMAT® IM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Melt Temperature 220 - 235 °C
428 - 455 °F
Lavergne VYTEEN ABS 2904 Acrylonitrile Butadiene Styrene
Vyteen ABS 2904 is a black recycled ABS high impact flow terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Excellent resilience -Good proc..
Melt Temperature 180 - 235 °C
356 - 455 °F
Injection
Styrolution Styrolux® GH 58 SBC
Description: Styrolux® GH 58 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warp..
Melt Temperature 225 - 235 °C
437 - 455 °F
Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications
Borcoat BB700E-7032 is a grey colored high impact polypropylene. This product is especially designed for direct extrusion of syntactic PP with high thermal insulations capacity and high compression..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E781 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 21E830 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate
BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 4140 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E755 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E725 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E806 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Melt Temperature 160 - 235 °C
320 - 455 °F
Blown/Cast Film Coextrusion
DuPont™ Elvaloy® AC 1330 Ethylene Methyl Acrylate
Elvaloy® AC 1330 is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A..
Melt Temperature 215 - 235 °C
419 - 455 °F
Celanese RITEFLEX 663 TPC, Unfilled
Riteflex 663 is a nominal 63 Shore D thermoplastic polyester elastomer with medium modulus.Information provided by Celanese
Melt Temperature 225 - 235 °C
437 - 455 °F
V400P LCP, Specialty
Co-extrudable LCP for Barrier Applications. V400P Liquid Crystal Polymer is characterized by its excellent barrier properties independent of relative humidity, chemical resistance and contact clari..
Melt Temperature 180 - 235 °C
356 - 455 °F
Injection Molding
BASF Styroclear GH 58 SBC
Styroclear GH 58 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warpage resistance..
Melt Temperature 205 - 235 °C
401 - 455 °F
Celanese RITEFLEX 655HS TPC, Unfilled
55 Shore D Hardness heat stabilizedInformation provided by Celanese
Melt Temperature 225 - 235 °C
437 - 455 °F
LookPolymersN™ V300P Co-Extrudable Liquid Crystal Polymer (LCP)
Description: PRELIMINARY DATA SHEET: Co-extrudable LCP for Barrier Applications. V300P Liquid Crystal Polymer is characterized by its low processing temperature, excellent barrier properties indepe..
Melt Temperature 227 - 235 °C
441 - 455 °F
LNP Thermocomp® SF-1006 Polyamide 12, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Copyright © lookpolymers.com All Rights Reserved