Processing Properties Metric English Comments
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 1600A PBT  (Unverified Data**)
Celanex 1600A is a high molecular weight grade of unreinforced polybutylene terephthalate used in both extrusion and injection molding applications.Extrusion gradeInformation provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 1700A PBT  (Unverified Data**)
Celanex 1700A is a very high molecular weight grade of unreinforce polybutylene terephthalate for extrusion applications.Highest molecular weightInformation provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 2008 PBT  (Unverified Data**)
Celanex 2008 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Ultrahigh melt flowInfor..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 2104UV PBT, UV Resistant  (Unverified Data**)
Celanex 2104UV is an unreiforced, impact modified, UV stabilized PBT designed for outdoor agricultural, industrial and automotive applications. Celanex 2104UV is suitable for injection molding appli..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300LM is a 30% glass reinforced PBT that is enhanced for improved laser marking graphics. 3300LM also offers a superior combination of mechanical, electrical, and thermal properties. This g..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 4022 PBT, Specialty  (Unverified Data**)
A white PBT resin typically used for applications requiring very opaque parts.PBT, opaque whiteInformation provided by Celanese
Zone 3 235 - 255 °C
455 - 491 °F
Celanese Celanex® 6400-2 PBT, Mineral / Glass Reinforced  (Unverified Data**)
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.40% glass/mineral filled, low warpInformation provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Vandar® 8000 PBT  (Unverified Data**)
Vandar 8000 polyester alloy is designed to meet UL94 V-0 requirements at 1/32 inch thickness while retaining excellent impact resistance. The product is characterized by excellent moldability and su..
Zone 3 235 °C
455 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Zone 3 235 °C
455 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Zone 3 235 °C
455 °F
CoExtrusion with EVOH Processing
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 1400A PBT, Unfilled
Celanex 1400A is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1400A is a high flow material.Information provide..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 2016 PBT, Unfilled
Celanex 2016 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), unreinforced polybutylene terephthalate which has an excellent balance of mechanical propertie..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 2401 MT PBT, Medical Technology
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3309HR PBT, 30% Glass Reinforced
Celanex 3309HR is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.Information provided by C..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese CELANEX 4309AR PBT
Celanex 4309AR is a 30% glass reinforced PBT with enhanced resistance to hydrolysis, alkaline environments and salt water spray.Information provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 4305 PBT, 33% Glass Reinforced
Celanex 4305 is a 33% glass reinforced, toughened, thermoplastic polyester.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less tha..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 602AC PBT, Glass Reinforced
Celanex 602AC is a 10% fiberglass reinforced PBT that has lower warpage and improved impact over standard PBT.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a ..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 7316 PBT, 35% Mineral / Glass Reinforced
Celanex 7316 is a non-exuding (UL and CSA approved V-0 at 1/32 inch), 35% glass/mineral reinforced PBT, which has an excellent balance of mechanical properties and processability. It is well suited..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese VANDAR 4602Z PBT, Unfilled
4602Z is an unfilled thermoplastic alloy with good weatherability and chemical resistance.Information provided by Celanese
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 2002UV PBT, Unfilled
Celanex 2002UV is a general purpose,unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability and UV resistance. Celanex 2002UV is a medium flow materialTo..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3225HRT PBT, 15% Specialty
Celanex 3225HRT is a non-lubricated, 15% fiberglass reinforced Polybutylene Terphthalate copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at brea..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3309HRHF PBT, 30% Glass Reinforced
Celanex 3309HRHF is a 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and improved flow.Information provided by Celanese Corpora..
Zone 3 235 - 255 °C
455 - 491 °F
Celanese Celanex® 5300-2UV PBT, 30% Glass Reinforced
Information provided by Celanese Corporation.
Zone 3 235 - 255 °C
455 - 491 °F
Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced
Celanex 6406 is a 40% mineral/glass reinforced resin providing excellent toughness combined with warpage resistance, surface gloss and good mechanical properties. Celanex 6406 is particularly suited..
Zone 3 235 - 250 °C
455 - 482 °F
Celanese Celanex® 1400FC PBT  (Unverified Data**)
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Zone 3 235 - 255 °C
455 - 491 °F
Celanese Celanex® 6407 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6407 is a 30% glass/mineral reinforced resin perticularly suited for large exterior automotive components, where extended flow, flatness and good surface appearance is essential.30% glass/mi..
Zone 3 235 - 255 °C
455 - 491 °F
Celanese Celanex® J600 PBT, 40% Mineral / Glass Reinforced  (Unverified Data**)
Celanex J-600 is a 40% glass/mineral reinforced resin providing excellent warpage resistance, surface gloss and good mechanical properties. Celanex J-600 is particularly suited to applications requi..