Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 235 °C | 455 °F | For film or coating with EVA or EVOH. |
DuPont Bynel® 21E553 Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |
|||
Die Temperature | 235 °C | 455 °F | |
DuPont Bynel® 30E699 Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Die Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 41E623 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Die Temperature | 235 °C | 455 °F | Extrusion Coating |
DuPont Appeel® LSR11N704 Lidding Sealant Resin
(discontinued **) Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal.. |
|||
Die Temperature | 235 °C | 455 °F | |
DuPont Bynel® 30E671 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Die Temperature | 235 °C | 455 °F | |
DuPont Bynel® 39E660 Adhesive Resin Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Die Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 41E687 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Die Temperature | 235 °C | 455 °F | Extrusion Coating |
DuPont Appeel® LSR11D554 Lidding Sealant Resin Appeel® LSR11D554 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals to poly.. |
|||
Die Temperature | 235 °C | 455 °F | |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E781 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E830 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Die Temperature | 235 °C | 455 °F | Cast Film/Sheet Processing |
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Die Temperature | 235 °C | 455 °F | Cast Film/Sheet Processing |
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E850 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E725 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E806 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Die Temperature | 235 °C | 455 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® 1706 Zinc Ionomer Surlyn® 1706 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |
|||
Die Temperature | 235 °C | 455 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® 1707 Sodium Ionomer Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |
|||
Die Temperature | 235 °C | 455 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® 2601B Sodium Ionomer Surlyn® 2601B is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer .. |
|||
Die Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 50E662 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E662 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion an.. |
|||
Die Temperature | 235 °C | 455 °F | Extrusion Coating |
DuPont Appeel® LSR11D625 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D625 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals .. |