Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon

Category Polymer , Thermoplastic , Nylon
Manufacturer Cast Nylons Limited
Trade Name Nycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and laurinlactam, NYCAST® CP was originally developed specifically for use in ball valve seats in the oil and gas industry.NYCAST®CP with its higher elongation, superior dimensional stability and safety yellow color has found itself a superior choice for wobbler box inserts and coupling boxes in the cold rolling steel industry and mandrels covers in paper tube manufacturing plants.Data provided by the manufacturer, Cast Nylons Limited.
Physical Properties Metric English Comments
Density 1.10 - 1.13 g/cc
0.0397 - 0.0408 lb/in³
ASTM D792
Water Absorption 0.50 - 0.60 %
0.50 - 0.60 %
24 hrs; ASTM D570
Water Absorption at Saturation 4.0 - 5.0 %
4.0 - 5.0 %
ASTM D570
Deformation 0.40 - 0.80 %
0.40 - 0.80 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100 - 115
100 - 115
ASTM D785
Hardness, Shore D 75 - 81
75 - 81
ASTM D2240
Tensile Strength 60.0 - 79.3 MPa
8700 - 11500 psi
ASTM D638
Elongation at Break 25 - 80 %
25 - 80 %
ASTM D638
Tensile Modulus 1.65 - 2.28 GPa
240 - 330 ksi
ASTM D638
Flexural Strength 103 - 138 MPa
15000 - 20000 psi
ASTM D790
Flexural Modulus 1.97 - 2.65 GPa
285 - 385 ksi
ASTM D790
Compressive Strength 75.8 - 86.2 MPa
11000 - 12500 psi
ASTM D695
Compressive Modulus 1.38 - 2.07 GPa
200 - 300 ksi
ASTM D695
Shear Strength 52.4 - 62.1 MPa
7600 - 9000 psi
ASTM D732
Izod Impact, Notched 0.481 - 0.747 J/cm
0.900 - 1.40 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.22
0.22
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Melting Point 204 - 216 °C
400 - 420 °F
Maximum Service Temperature, Air 98.9 °C
210 °F
Continuous
149 °C
300 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
400 - 430 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.3 - 204 °C
200 - 400 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 60.0 Hz
3.7

@Frequency 60.0 Hz
ASTM D150
3.7

@Frequency 1000 Hz
3.7

@Frequency 1000 Hz
ASTM D150
3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 19.7 - 23.6 kV/mm
500 - 600 kV/in
ASTM D149