Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Quadrant EPP Nylatron® 703 XL Cast, Wear Resistant, Zero 'Stick-Slip' (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Quadrant EPP Nylatron® GSM Blue Nylon, Cast Oil & MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Quadrant EPP Nylatron® LIG Oil Filled Cast 6 Nylon (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Quadrant EPP Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Broadest size range availability Good mechanical and electrical properties Ideal balance of strength and toughness Cast as finished parts and n.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Polymer Resources PPX-FR2-[color]EN Modified PPO, UL 94 V-1 with HDT of 210 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Polymer Resources PPX-FR2-[color]-EN Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)& Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | Unannealed, 0.125 in bars; ASTM D648 |
PolyOne Lubri-Tech™ NL-15KV/000 Nylon 6/12, Aramid Fiber
(discontinued **) Description/Features:Aramid Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS GF15 FR-2 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ABS GF20 FR RD073 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Flame RetardantAppearance: RedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HIPS GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® HIPS GF50 50% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | unannealed, .125in; ASTM D648 |
Star Plastics ABSGF10 Molding Grade ABS With 10% Glass Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | unannealed, .125in; ASTM D648 |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | unannealed, .125in; ASTM D648 |
Star Plastics PC/PBT7804 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Techmer ES Plaslube® NY-1/TF/15 NAT PA66 |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® ABS TX15 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(15%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Techmer ES Plaslube® NY-1/MS/5 BK223 PA66 |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Ecomass® 1850ZD88 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Ensinger Tecast Vekton™ 6XAU High Heat Cast Nylon 6 (PA6) VEKTON® 6XAU is a high heat weather resistant cast nylon 6 with superior fatigue-resistant and bearing properties.General Vekton® Cast Nylon Information: VEKTON cast nylon, available in a variety .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 |
Diamond Polymers ABS 3002MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Ensinger Tecast Vekton™ 6PAM MoS2-Filled Cast Nylon 6 (PA6) Tecast® 6PAM is a molybdenum disulfide-filled cast nylon 6 used for general bearings and wear applications and for its superior strength and hardness.General Tecast® Cast Nylon Information: Tecast.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
Polymer Resources PPX-FR2 Modified PPO, UL 94 V-1 with HDT of 210 F