Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.97 GPa | 286 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6 PA6 IM20 Unfilled/ Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6/6 PA6/6 IM20 Unfilled/ Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 25-0105 TF20 Description: Copolymer Polypropylene, 20% Talc FilledInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | ASTM D790 |
Ineos Nova FX510 Super High Impact Polystyrene
(discontinued **) Features: Extremely high impact strengthGood flexural strengthUL Classification 94 HBCustom colors availableApplications: Injection molding or extrusionSuitable replacement for some engineering resi.. |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | 0.1 in/min; ASTM D790 |
Ineos Nova 1983 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Color Stable, Custom colors, UL94 HB at 0.060 for all colorsApplications: Suitable for extrusion or injection molding processes requiring.. |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | ISO 178 |
Aardvark Polymers AARTEL® 850IM Rotational Molding Resin Aartel 850 IM is a moderately toughened impact modified acetal copolymer which exhibits ductility in bending and impact loading. The ductile, rather than brittle, failure mode gives designers more f.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
Kostat ICP-STAT ICS-1001 PET Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
Kostat ICP-STAT ICD-1001 PET Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | tangent; ASTM D790 |
Spartech PP5220 Calcium Carbonate Filled Homopolymer Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | tangent; ASTM D790 |
Spartech PP5312 Mica Reinforced Homopolymer Information provided by Spartech |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
Star Plastics PC/PBT7804 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D 790 |
Styrolution PS 7800 HIPS Extremely high surface glossGood processabilityUL Classification 94 HBInformation provided by Styrolution |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL HIPS3190 HIPS Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | Tangent; ASTM D790 |
Washington Penn Medium Impact Copolymer 20% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
American Polymers API 410 Polystyrene API 410 is a low impact polystyrene with very high gloss and superior dimensional stability.Applications: API 410 is ideally suited for point of purchase displays where high gloss and some impact i.. |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | ASTM D790 |
Ecomass® 3608TU96 Tungsten Filled Polyethylene Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyethylene (HDPE)Information provided by Technical Polymers |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 7502 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 7501 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.97 - 2.65 GPa | 285 - 385 ksi | ASTM D790 |
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | ASTM Test |
BASF Ultraform N 2640 Z2 UNC Q600 POM Ultraform N2640 Z2 UNC Q600 is an elastomer-modified grade of POM for injection molding with high impact strength. |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | ASTM Test |
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Conditioned) Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the.. |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | ASTM D790 |
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma.. |
|||
Flexural Modulus | 1.97 GPa | 286 ksi | ASTM D790 |
Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |