Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 75.8 - 86.2 MPa | 11000 - 12500 psi | ASTM D695 |
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |