Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Polimeri Europa Edistir ICE R 830D Polystyrene Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Polimeri Europa Edistir R 850E Polystyrene Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injecti.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
dry sample |
Omnia Plastica Omniamid PA 6 - Akulon 6 - at 50% RH Semi-crystalline polymer of polyamide obtained by the polymerisation of the caprolactam. Its large popularity is due to both its good overall features as well as its cost-performance relationship. T.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Polimeri Europa Sinkral® B 532/E ABS Resin Sinkral B 532/E is an extrusion grade, which combines high toughness with good rigidity. Its rheological characteristics and good thermal stability are required for the production of large extruded .. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Polycasa XT 630 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 23.0 - 100 °C |
50.0 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data) This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 23.0 - 100 °C |
50.0 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data) The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybd.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | |
Permabond HM160 Anaerobic Retaining Compound Permabond® HM160 is a medium viscosity liquid adhesive that cures when confined between metal parts to form a tough, hard plastic. In the uncured, liquid state, the adhesive wets the metal surfaces.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | |
Permabond LH050 Anaerobic Threadsealant Permabond® LH050 pipe sealant with PTFE is a general purpose pipe sealant that provides instant air pressure seal up to 1000 psi with limited hand tightening. After cure, the sealing capability is .. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | |
Permabond LH056 Anaerobic Threadsealant Permabond LH056 is a thread sealant designed for use in sealing metal pipes and fittings in sprinkler systems which may also contain CPVC piping. Permabond LH056 prevents leaks even on pipes that ar.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | |
Permabond 791 Cyanoacrylate, Surface insensitive PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | |
Permabond F201 Anaerobic Retainer Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,.. |
|||
CTE, linear | 90.0 - 150 µm/m-°C | 50.0 - 83.3 µin/in-°F | Average value: 113 µm/m-°C Grade Count:7 |
Overview of materials for Nylon 11, Flexible Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 80-7718 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM-D696 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM E831 |
Lucite International Diakon® TD510 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Soft Touch ASA/ABS Co-Extruded Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech SP-9010 General Purpose ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359 |
Styrolution Novodur® M203FC ABS Novodur HD M203FC is an injection molding grade especially suitable for medical applications providing high flowability.Information provided by Styrolution |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359 |
Styrolution Novodur® M210TF ABS Novodur M210TF is medium impact, high gloss injection molding grade designed for toy application. M210TF is in compliance with food contact regulationsInformation provided by Styrolution |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Samyang Tribit® 1501N PBT, Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1501N is a V-2 flame retardancy grade.Appli.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
CENTROPLAST CENTROMID 6 E Polyamide 6 extruded This tough and impact resistant material has good chemical resistance and can be bonded and welded. It is used for sealing rings, flanges, etc. Information provided by CENTROPLAST Engineering Plast.. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Americas Styrenics STYRON® 610 High Heat Crystal Polystyrene Product CharacteristicsAdditive freeTypical ApplicationsFoamsFilms/opticalCarrier resinSpecialty blendingInformation provided by AmericasStyrenics LLC. |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Americas Styrenics STYRON® 695 High Heat Crystal Polystyrene Product CharacteristicsReduced residualsHigh heat resistancehigh strengthFood Contact CompliantTypical ApplicationsOPSInformation provided by AmericasStyrenics LLC. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
50.0 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® A0100 PPE/PA AutomotiveInformation provided by Asahi Kasei |
|||
CTE, linear | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Gromax PBT 1200-211D Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® GB-25 Acetal Co-polymer (POM), Low warpage, GB 25% filling DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |