Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | ASTM D648 |
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | ASTM D648 |
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | ASTM D648 |
Polymer Resources TP-GFMF1 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame Retardant Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | ASTM D648 |
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Lubri-Tech™ NL-30GF/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)Information provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 399 °F | ISO 75-1/-2 |
Lanxess Durethan® TP 140-009 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade, 15% glass fibers, elastomer-modified, good heat-ageing resistance, dry-impact modified |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C @Thickness 3.20 mm |
399 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/6 IM5 BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 399 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C @Thickness 6.40 mm |
399 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 457 PBT 6.5% GR PBT, UL94 V-0/5V. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C @Thickness 6.40 mm |
399 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 553 PBT+PC (Asia Pacific) 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GB20 L 20% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF40 L 40% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Comp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C @Thickness 6.40 mm |
399 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA (Asia Pacific) 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 400 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6/66 IM3 BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection Moldi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 399 °F | ASTM D648 |
Adell BJ-34 Nylon 6, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 - 221 °C | 399 - 430 °F | ASTM D648 |
Cast Nylons Nycast® 6MPY Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPY is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 - 221 °C | 399 - 430 °F | ASTM D648 |
Cast Nylons Nycast® 6PA-Blue Nylon 6 NYCAST® 6 PA-Blue along with NYCAST® 6 PA-Natural have replaced bronze, brass, steel, and aluminum in various mechanical applications.Data provided by the manufacturer, Cast Nylons Limited.The dat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 - 221 °C | 399 - 430 °F | ASTM D648 |
Cast Nylons Nycast® 6PA-MoS2 Nylon 6 NYCAST® 6PA-MoS2 is a molybdenum disulphide filled Type 6 cast nylon. Finely divided MoS2 particles are suspended in the melt during polymerization. This gives the NYCAST® 6PA-MoS2 products improv.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 - 221 °C | 400 - 430 °F | ASTM D648 |
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 - 221 °C | 399 - 430 °F | ASTM D648 |
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 399 °F | ASTM D648 |
A. Schulman ComAlloy Lubrilon® 606 Nylon 6/6, PTFE Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 204 °C | 399 °F | ASTM D648 |
A. Schulman ComAlloy Lubrilon® 610 Nylon 6, Carbon Fiber/PTFE Reinforced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |