Mechanical Properties Metric English Comments
Compressive Strength 75.8 - 86.2 MPa
11000 - 12500 psi
ASTM D695
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon
Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau..