Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.97 GPa | 285 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 25-0105 TF20 Description: Copolymer Polypropylene, 20% Talc FilledInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
Kostat ICP-STAT ICS-1001 PET Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
Kostat ICP-STAT ICD-1001 PET Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | tangent; ASTM D790 |
Spartech PP5220 Calcium Carbonate Filled Homopolymer Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | tangent; ASTM D790 |
Spartech PP5312 Mica Reinforced Homopolymer Information provided by Spartech |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
Star Plastics PC/PBT7804 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D 790 |
Styrolution PS 7800 HIPS Extremely high surface glossGood processabilityUL Classification 94 HBInformation provided by Styrolution |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | Tangent; ASTM D790 |
Washington Penn Medium Impact Copolymer 20% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
American Polymers API 410 Polystyrene API 410 is a low impact polystyrene with very high gloss and superior dimensional stability.Applications: API 410 is ideally suited for point of purchase displays where high gloss and some impact i.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 7502 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 7501 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.97 - 2.65 GPa | 285 - 385 ksi | ASTM D790 |
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |
|||
Flexural Modulus | 1.97 GPa | 285 ksi | ASTM D790 |
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |