Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ecovio® C2203 F Blend Biodegradable Polyester

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polylactic Acid (PLA) Biopolymer
Manufacturer BASF
Trade Name Ecovio®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ecovio® C2203 F Blend Biodegradable Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic acid (PLA). Because of the PLA content Ecovio® F Blend C2203 consists of 32% of renewable resources. Ecoflex® F Blend is the conitnuous phase in the structure of Ecovio® F Blend C2203 transferring the beneficial film properties of Ecoflex® F Blend into the new product.Application: Ecovio® F Blend C2203 has been developed for the conversion to flexible films using a blown film process. Typical applications are packaging films, hygienic films, carrier bags and compost bags. In view of numerous factors influencing functionality and shelf life of Ecovio® films and finished articles made therof the production parameters have to be tested by the converters before utilization. Additionally sufficient field tests are required to ensure the right functionality of the articles made from Ecovio® F Blend C2203.Information provided by BASF
Physical Properties Metric English Comments
Density 1.24 - 1.26 g/cc
0.0448 - 0.0455 lb/in³
ISO 1183
Water Vapor Transmission 84.0 g/m²/day
5.41 g/100 in²/day
ASTM F1249
Oxygen Transmission Rate 670 cc/m²/day
43.1 cc/100 in²/day
dry; ASTM D3985
Melt Flow <= 2.0 g/10 min
<= 2.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ISO 868
Tensile Strength 30.0 - 39.0 MPa
4350 - 5660 psi
ISO 527
Tensile Strength, Ultimate 29.0 - 39.0 MPa
4210 - 5660 psi
ISO 527
Elongation at Break 330 - 430 %
330 - 430 %
ISO 527
Tensile Modulus 0.280 - 0.840 GPa
40.6 - 122 ksi
ISO 527
Dart Drop Total Energy 420 J/cm
0.787 ft-lb/mil
DIN 53373
Thermal Properties Metric English Comments
Melting Point 110 - 120 °C
230 - 248 °F
DSC
140 - 155 °C
284 - 311 °F
DSC
Vicat Softening Point 70.0 °C
158 °F
A/50; ISO 306
Optical Properties Metric English Comments
Haze 85 %
85 %
ASTM D1003
Descriptive Properties Value Comments
Commercial Status Europe