Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 70.0 °C @Load 5.10 kg |
158 °F @Load 11.2 lb |
ISO 306 |
SABIC P5510 Black High Density Polyethylene for Pipes Product Description: P5510 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50°C/hr; 50N |
Polimeri Europa KOBLEND PD P476B PS+PE, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: (S/B + PE) Special polystyrene alloy with very high tear strength and high stress- cracking resistances. Particularly suitable for extrusion and thermoforming of fat.. |
|||
Vicat Softening Point | 70.0 - 150 °C | 158 - 302 °F | Average value: 112 °C Grade Count:9 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® TPU-7682 Thermoplastic polyurethane, with carbon fiber Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Mitsui ADMER® NF908A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Lushan M-10D Adhesive Resin for Multi-layer Sausage Casing film Adhesive resin Lushan series for sausages casing film is anhydride-modified polyethylene product and is available in pellet form. Adhesive resin Lushan series for sausages casing film is designed fo.. |
|||
Vicat Softening Point | 70.0 °C @Load 5.00 kg |
158 °F @Load 11.0 lb |
|
LATI Latene® EP 7 TES/30 PP Copolymer, 30% Talc filled Polypropylene copolymer (PPc) based compound. Aesthetic talc. Very good surface appearance. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo.. |
|||
Vicat Softening Point | 70.0 °C @Load 5.00 kg |
158 °F @Load 11.0 lb |
|
LATI Latene® EP 7-V2 PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Vicat Softening Point | 70.0 °C @Load 5.00 kg |
158 °F @Load 11.0 lb |
|
LATI Latilub 45/7-20T HDPE, PTFE Reinforced Self-lubricating product based on High density polyethylene (HD-PE). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Lushan M-2 Adhesive Resin for Barrier Container and Tube Adhesive resin Lushan series for barrier container and tube is used for bonding a wide variety of materials, It’s most often used to adhering PE and EVOH, PP and EVOH, etc. Adhesive resins Lush.. |
|||
Vicat Softening Point | <= 70.0 °C | <= 158 °F | |
Sibur ABS-TB (30,31) Molding Grade ABS Plastic With high fluidity of melting, thermal and light resistance for large parts of devices, parts of refrigerators, and for hearing aids. Mark is allowed for contact with food products. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
SK Chemicals SKYTHANE® CR180A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
SK Chemicals SKYTHANE® R180A C series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Lubrizol Estane® T460AH Thermoplastic Polyurethane Type: Estane® T460AH is a Shore 60A, polyester grade, plasticizer-free, with low hardness and Hydrolytic Stabilizer thermoplastic polyurethane (TPU).Uses: Injection Molding.Availability: Americas, .. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
UBE V115 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 9760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9760 is heterophasic copolymer. PPC 9760 is characterized by improved stiffness, creep resistance and high impact resistance. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Lubrizol Estane® CR180A Thermoplastic Polyurethane Type: Estane® CR180A is a Shore 82A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | B (50N); ISO 306 |
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 12712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 4640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4640 is a nucleated copolymer. PPC 4640 is characterized by good stiffness and impact resistance coupled with high creep resistance. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane Features: Displays Low Temperature Flexibility and Abrasion Resistance.Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for LaminationAvailable in Americas and AsiaInfo.. |
|||
Vicat Softening Point | 70.0 °C @Load 0.999 kg |
158 °F @Load 2.20 lb |
ASTM D1525 |
Arkema Group LOTADER® 6200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 6200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties (reactivity, fluidity), LOTADER 62.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ASTM D1525 |
Arkema Group Orevac® 9314 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Blown film coextrusionInformation provided by Arkema Group |
|||
Vicat Softening Point | 70.0 °C | 158 °F | 50N-50°C per hour; ISO 306 |
Total PPC 10712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 10712 is a nucleated and controlled-rheology heterophasic copolymer. PPC 10712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. |
|||
Vicat Softening Point | 70.0 - 72.0 °C @Load 5.00 kg |
158 - 162 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RI 548/H Rigid PVC, Antishock Injection Molding Electric antishock fittings |
|||
Vicat Softening Point | 70.0 °C | 158 °F | ISO 306 |
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym.. |
|||
Vicat Softening Point | 70.0 °C | 158 °F | A/50; ISO 306 |
BASF Ecovio® C2203 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |