Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.280 - 0.840 GPa | 40.6 - 122 ksi | ISO 527 |
BASF Ecovio® C2203 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |