Polymer Property : Density = 1.26 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.10 - 1.26 g/cc
0.0397 - 0.0455 lb/in³
Average value: 1.17 g/cc Grade Count:6
Overview of materials for PPE/PPO + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr..
Density 1.07 - 1.26 g/cc
0.0387 - 0.0455 lb/in³
Average value: 1.12 g/cc Grade Count:17
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Density 1.19 - 1.26 g/cc
0.0430 - 0.0455 lb/in³
Average value: 1.20 g/cc Grade Count:55
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Density 1.23 - 1.26 g/cc
0.0444 - 0.0455 lb/in³
322 Hardener
Lord Adhesives 320 / 322 Epoxy Adhesive
LORD® 320/322 adhesive is a general purpose, two component epoxy adhesive system formulated for primerless adhesion to automotive sheet molded compounds (SMC). This adhesive system also provides ..
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds GS 6802 Flexible PVC, Injection Molding for Footwear
Soles
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds GS 7010 Flexible PVC, Injection Molding for Footwear
Soles
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds GS 7303 Flexible PVC, Injection Molding for Footwear
Soles
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds GS 75/O Flexible PVC, Injection Molding for Footwear
Heels, opaque surface
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds GS 89/T Flexible PVC, Injection Molding for Transparent Technical Items
Technical items
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds GS 6612 Flexible PVC, Injection Molding for Footwear
Soles
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds MGS 91/T Medical Flexible PVC, Injection Molding
Connectors and special components
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1184
Fainplast Compounds MPH 87 Medical Flexible PVC, Extrusion
Tubolar apparatus
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds PH 60/AS Flexible PVC, Transparent Extrusion
Food belt carriers
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds PH 74/AL Flexible PVC, Transparent Extrusion
Profiles according to CEE 90/128
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds PH 83 Flexible PVC, Transparent Extrusion
Transparent profiles and pipes
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds PM 5526/1 Flexible PVC, Lead Free
Gaskets for frames
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds PM 7010/K Flexible PVC, Lead Free
Pipes
Density 1.24 - 1.26 g/cc
0.0448 - 0.0455 lb/in³
ISO 1183
BASF Ecovio® C2224 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1184
Fainplast Compounds KLT 002 Flexible PVC, Insulation Transparent Cables Lead Free
Transparent cables (105°C)
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1184
Fainplast Compounds KLT 90/UV Flexible PVC, Sheathing Transparent Cables Lead Free
Transparent cables anti-UV
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds MGS 86 Medical Flexible PVC, Injection Molding
Connectors and special components
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1184
Fainplast Compounds MPH 81 Medical Flexible PVC, Extrusion
Tubolar apparatus
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds PM 6510/K Flexible PVC, Lead Free
Pipes, UL 94 Class V1
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds PM 6710 Flexible PVC, Lead Free
Gaskets for frames
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds PM 7005 Flexible PVC, Lead Free
Pipes and profiles
Density 1.14 - 1.26 g/cc
0.0412 - 0.0455 lb/in³
Average value: 1.20 g/cc Grade Count:5
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is ..
Density 1.22 - 1.26 g/cc
0.0441 - 0.0455 lb/in³
ISO R 1183
Fainplast Compounds PM 65/7 Flexible PVC, Lead Free
Fuses
Density 1.24 - 1.26 g/cc
0.0448 - 0.0455 lb/in³
ISO 1183
BASF Ecovio® C2203 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..